Polyether-block-amide (PEBA) /clay nanocomposites were prepared water-assisted by twin-screw extrusion. Both organomodified and pristine (i.e. purified but non-modified) montmorillonite clays were used. A high-pressure differential scanning calorimetry analysis carried out in the processing conditions demonstrated that PEBA/water blend exhibits some miscibility and that amide blocks and water behave as a single phase. In addition to a significant decrease of the melting temperature, water injected into the melt plays a key role among the filler dispersion and prevents the matrix from degradation during melt-extrusion. This process enables the compounding of pristine clay-based nanocomposites whose dispersion state is high enough for the resulting mechanical performances in tension to be at least equivalent to what is reached with organomodified clay. Effects of the nanofiller dispersion onto the macromolecules’ mobility are detailed and fracture mechanisms are identified for the various structures
A remarkable synergistic increase in fracture toughness by 130% is demonstrated for a CFRP high performance epoxy composite when adding an equal weight combination of phenoxy thermoplastic and core-shell rubber (CSR) toughening agents, as compared to a single toughener at a comparable total concentration of around 10 wt%. The dual-toughened matrix exhibits an unusual morphological arrangement of the two toughener agents. The interlaminar shear strength of the composites is also synergistically improved by about 75% as compared to the reference while the compression modulus reduction and viscosity increase are significantly smaller than for the single phenoxy toughened system. A partial filtering of the CSR particles by the dense CF fabric during pre-pregging leads to a less than optimum CSR dispersion in the composites, showing that the synergy can be further optimized, possibly to the same level as the unreinforced systems.
A major societal issue of disposal and environmental pollution is raised by the enormous and fast-growing production of single-use polyethylene terephthalate (PET) bottles, especially in developing countries. To contribute to the problem solution, an original route to recycle PET in the form of value-added environmentally friendly thermoplastic composites with banana fibres (Musa acuminata) has been developed at the laboratory scale. Banana fibres are a so far undervalued by-product of banana crops with great potential as polymer reinforcement. The melt-processing constraints of commercial PET, including used bottles, being incompatible with the thermal stability limits use of natural fibres; PET has been modified with bio-sourced reactants to produce co-polymers with moderate processing temperatures below 200 °C. First, commercial PET were partially glycolyzed with 1.3-propanediol to produce co-oligomers of about 20 repeating units, which were next chain extended with succinic anhydride and post-treated in a very unusual “soft solid state” process at temperatures in the vicinity of the melting point to generate co-polymers with excellent ductility. The molar mass build-up reaction is dominated by esterification of the chain ends and benefits from the addition of succinic anhydride to rebalance the acid-to-hydroxyl end-group ratio. Infra-red spectroscopy and intrinsic viscosity were extensively used to quantify the concentration of chain ends and the average molar mass of the co-polymers at all stages of the process. The best co-polymers are crystallisable, though at slow kinetics, with a Tg of 48 °C and a melting point strongly dependent upon thermal history. The composites show high stiffness (4.8 GPa at 20% fibres), consistent with the excellent dispersion of the fibres and a very high interfacial cohesion. The strong adhesion can be tentatively explained by covalent bonding involving unreacted succinic anhydride in excess during solid stating. A first approach to quantify the sustainable benefits of this PET recycling route, based on a rational eco-selection method, gives promising results since the composites come close to low-end wood materials in terms of the stiffness/embodied energy balance. Moreover, this approach can easily be extended to many other natural fibres. The present study is limited to a proof of concept at the laboratory scale but is encouraging enough to warrant a follow-up study toward scale-up and application development.
Flexible thermoelectric devices based on interconnected networks of bismuth nanowires embedded in nanoporous polymer films for thermal energy recovery in longitudinal and transverse geometries.
Arrays of thermoelectric nanowires embedded in organic films are attracting increasing interest to fabricate flexible thermoelectric devices with adjustable dimensions and complex shapes, useful for sustainable power sources of portable electronic devices and wireless sensor networks. Here, we report the electrochemical synthesis of interconnected bismuth-antimony (Bi1-xSbx) nanowires (with 0.06 < x < 0.15) within the branched cylindrical nanopores of polycarbonate membranes. The influence of temperature and magnetic field on the electrical and thermoelectric properties were studied by considering electric and thermal currents flowing in the plane of the films. We show that short annealing times up to 250○C of the nanowire-based nanocomposite leads to a large increase in the thermoelectric power, reaching values up to -80 μV/K at room temperature, which are comparable to those of bulk Bi-Sb alloys. In addition, we report Hall effect measurements on crossed nanowires, made possible for the first time by the remarkable electrical connectivity of the nanowire network. These measurements, combined with variations in temperature and under magnetic field of the electrical resistance, indicate that the interconnected networks of Bi1-xSbx nanowires after thermal annealing behave like n-type, narrow band gap semiconductors. Overall, the electrical and thermoelectric properties near ambient temperature of the heat-treated Bi1-xSbx nanowire networks are similar to those of bulk polycrystalline Bi-Sb alloys, which are well-known thermoelectric materials exhibiting optimal performance near and below room temperature.
The structure and properties of blends of a novel polyethylene terephthalate copolymer (COPET) obtained by chemical recycling of commercial PET with high-molar-mass poly-L-lactide (PLLA) are investigated and compared to corresponding composites with chopped flax fibres. The focus is on the morphology at nano- and micro-scales, on the thermal characteristics and on the mechanical behaviour. The blends are immiscible, as evidenced by virtually unchanged glass transition temperatures of the blend components compared to the neat polymers (49 °C for COPET and 63 °C for PLLA by DSC). At low PLLA content, the blends display a sea–island morphology with sub-micron to micron droplet sizes. As the composition approaches 50/50, the morphology transitions to a coarser co-continuous elongated structure. The blends and composites show strongly improved stiffness compared to COPET above its glass transition temperature, e.g., from melt behaviour at 60 °C for COPET alone to almost 600 MPa for the 50/50 blend and 500 MPa for the 20% flax composite of the 80/20 COPET/PLLA blend. The flax fibres increase the crystallisation rate of PLLA in blends with dispersed PLLA morphology. The evidence of cavitation on the fracture surfaces of blends shows that despite the immiscibility of the components, the interfacial adhesion between the phases is excellent. This is attributed to the presence of aliphatic ester spacers in COPET. The tensile strength of the 80/20 blend is around 50 MPa with a Young’s modulus of 2250 MPa. The corresponding 20% flax composite has similar tensile strength but a high Young’s modulus equal to 6400 MPa, which results from the individual dispersion and strong adhesion of the flax fibres and leads close to the maximum possible reinforcement of the composite, as demonstrated by tensile tests and nano-indentation. The Ashby approach to eco-selection relying on the embodied energy (EE) further clarifies the eco-friendliness of the blends and their composites, which are even better positioned than PLLA in a stiffness versus EE chart.