Porous mineralized collagen membranes efficiently promote bone regeneration. To generate them, we need to fabricate collagen membranes that are porous. However, the current fabrication method is primarily based on a bottom-up strategy, with certain limitations, such as a long manufacturing process, collagen denaturation, and failure to control fibril orientation. Using a top-down approach, we explore a novel method for constructing porous collagen membranes via the combined application of bioskiving and sonication. Numerous collagen membranes with well-aligned fibril structures were rapidly fabricated by bioskiving and then sonicated at 30, 60, 90, and 120 W for 20 min. This treatment allowed us to study the effect of power intensity on the physicochemical traits of collagen membranes. Subsequently, the prepared collagen membranes were immersed in amorphous calcium phosphate to evaluate the feasibility of mineralization. Additionally, the bioactivities of the membranes were assessed using preosteoblast cells. Tuning the power intensity was shown to modulate fibril orientation, and the porous membrane without denatured collagen could be obtained by a 20-min sonication treatment at 90 W. The prepared collagen membrane could also be further mineralized to enhance osteogenesis. Overall, this study offers a rapid and convenient approach for fabricating porous collagen membranes via bioskiving and sonication.
Purpose: To evaluate the influence of repetitive autoclaving on diamond burs fabricated via different methods. Materials and Methods: A total of 96 diamond burs were divided into 12 groups according to fabrication method (single-element electroplating, multi-element electroplating, or brazing) and number of times autoclaved (0, 5, 10, or 15). The surface characteristics and components of the diamond burs were examined using scanning electron microscopy (SEM) and x-ray photoelectron spectroscopy (XPS). The cutting efficiency of the diamond burs was tested with a constant-pressure cutting appliance. Results: Compared to the nonautoclaved group, the cutting efficiency of the multi-element and single-element electroplated diamond burs decreased significantly after autoclaving 5, 10, and 15 times (P < .05). The cutting efficiency of the brazed diamond burs started to decrease significantly after 10 cycles (P < .05). Cracks appeared on the surfaces of multi-element electroplated diamond burs after 10 and 15 cycles, but were absent in the single-element electroplated and brazed diamond burs. A reduction of nickel was detected in the multi-element electroplated and brazed diamond burs, but not in the single-element electroplated diamond burs. Conclusion: Repetitive autoclaving could reduce the cutting efficiency of diamond burs. The extent of the reduction was related to fabrication method and number of autoclaving times, suggesting that used diamond burs should be separately autoclaved to avoid shortening the life spans of unused ones.
17 June 2026 in European Journal of Dental Education