We have employed plasma-enhanced and thermal atomic layer deposition (ALD) within the temperature range of 50–150°C for the deposition of ultra-thin (10–50 nm) Al2O3 films on 100Cr6 steel and aluminium Al2024-T3 alloys. [Al(CH3)3] was used as the precursor with either an O2 plasma or water as co-reactants. Neutral salt spray tests showed that the thicker films offered the best corrosion-resistance. Using cyclic voltametry, the 50 nm films were found to be the least porous (<0.5%). For 10 nm thick films, plasma-enhanced ALD afforded a lower porosity and higher film density than thermal ALD. ToF-SIMS measurements on 100Cr6 showed that the main ‘bulk’ of the films contained very few impurities, but OH and C were observed at the interfaces. TEM confirmed that the films were conformal on all substrates and the adhesion was excellent for the films deposited by plasma-enhanced ALD but not for thermal ALD, as delamination was observed. On the basis of these and other results, the prospects of the application of ALD films for corrosion protection, and the use of plasma-enhanced ALD to promote their nucleation, is discussed.
15 January 2014 in ACS Applied Materials & Interfaces
Atomic layer deposited (ALD) aluminum and tantalum oxide (Al2O3 and Ta2O5) and their nanolaminates were applied as corrosion protection coatings on AISI 52100 steel. The aim was to combine the good sealing properties of Al2O3 with the chemical stability of Ta2O5 and to optimize the coating architecture in order to obtain the best possible long-term durability. Coating composition and morphology were studied with time-of-flight elastic recoil detection analysis (ToF-ERDA), time-of-flight secondary ion mass spectrometry (ToF-SIMS) and field emission scanning electron microscopy (FESEM) and energy dispersive x-ray spectrometry (EDS). Electrochemical properties were studied with voltammetry and electrochemical impedance spectroscopy (EIS), and corrosion durability with neutral salt spray (NSS) testing. The coatings were observed to be conformal and uniform over rough surfaces, and contained some carbon and hydrogen as impurities. The electrochemical results showed that the Al2O3 coating had superior sealing properties compared to the Ta2O5 coating, and nanolaminates had properties in between those of Al2O3 and Ta2O5. However, in the NSS test the laminate-coated samples survived the best demonstrating long-term durability. Analysis of the laminate structure showed that for 40 and 80 nm laminates the best protection was achieved with 10 and 20 nm layers, respectively.