Jebril Hadi

Dr. Jebril Hadi


Research Focus & Metrics

Academic Career Length

8Years (2019-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
15 April 2019 in Clays and Clay Minerals
Verified
Journal Article
Closed access
PDF file
JHJebril Hadi
Jebril Hadi
PWPaul Wersin
Paul Wersin
VSVincent Serneels
Vincent Serneels
JGJean-Marc Greneche
Jean-Marc Greneche
Corrosion of steel canisters containing buried high-level radioactive waste is a relevant issue for the long-term integrity of repositories. The purpose of the present study was to evaluate this issue by examining two differently corroded blocks originating from a full-scale in situ test of the FEBEX bentonite site in Switzerland. The FEBEX experiment was designed initially as a feasibility test of an engineered clay barrier system and was recently dismantled after 18 years of activity. Samples were studied by ‘spatially resolved’ and ‘bulk’ experimental methods, including Scanning Electron Microscopy, Elemental Energy Dispersive Spectroscopy (SEM-EDX), μ-Raman spectroscopy, X-ray Fluorescence (XRF), X-ray Diffraction (XRD), and 57Fe Mössbauer spectrometry, with a focus on Fe-bearing phases. In one of the blocks, corrosion of the steel liner led to diffusion of Fe into the bentonite, resulting in the formation of large (width > 140 mm) red, orange, and blue colored halos. Goethite was identified as the main corrosion product in the red and orange zones while no excess Fe2+ (compared to the unaffected bentonite) was observed there. Excess Fe2+ was found to have diffused further into the clay (in the blue zones) but its speciation could not be unambiguously clarified. The results indicate the occurrence of newly formed octahedral Fe2+ either as Fe2+ sorbed on the clay or as structural Fe2+ inside the clay (following electron transfer from sorbed Fe2+). No other indications of clay transformation or newly formed clay phases were found. The overall pattern indicates that diffusion of Fe was initiated when oxidizing conditions were still prevailing inside the bentonite block, resulting in the accumulation of Fe3+ close to the interface (up to three times the original Fe content), and continued when reducing conditions were reached, allowing deeper diffusion of Fe2+ into the clay (inducing an increase of 10–12% of the Fe content).

22 August 2021 in Minerals
Verified
Journal Article
Open access
PDF file
PWPaul Wersin
Paul Wersin
JHJebril Hadi
Jebril Hadi
AJAndreas Jenni
Andreas Jenni
DSDaniel Svensson
Daniel Svensson
JGJean-Marc Greneche
Jean-Marc Greneche
OLOlivier X. Leupin
Olivier X. Leupin
Bentonite, a common smectite-rich buffer material, is in direct contact with corroding steel in many high-level radioactive waste repository designs. The interaction of iron with the smectite-rich clay may affect its swelling and sealing properties by processes such as alteration, redox reactions and cementation. The chemical interactions were investigated by analysing the Fe/clay interfaces of eight bentonite blocks which had been exposed to temperatures up to 130 °C for five years in the ABM2 borehole at the Äspö Hard Rock Laboratory managed by the Swedish Nuclear Fuel and Waste Management Co (SKB). Eleven interface samples were characterised by high spatial resolution methods, including scanning electron microscopy coupled with energy dispersive X-ray spectroscopy and μ-Raman spectroscopy as well as by “bulk” methods X-ray diffraction, X-ray fluorescence and 57Fe Mössbauer spectrometry. Corrosion induced an iron front of 5–20 mm into the bentonite, except for the high-Fe bentonite where no Fe increase was detected. This Fe front consisted mainly of ferric (oxyhydr)oxides in addition to the structural Fe in the smectite fraction which had been partially reduced by the interaction process. Fe(II) was also found to extend further into the clay, but its nature could not be identified. The consistent behaviour is explained by the redox evolution, which shifts from oxidising to reducing conditions during the experiment. No indication of smectite alteration was found.

1 October 2023 in Clays and Clay Minerals
Verified
Journal Article
Open access
PDF file
JHJebril Hadi
Jebril Hadi
JGJean-Marc Greneche
Jean-Marc Greneche
PWPaul Wersin
Paul Wersin
PKPetri Koho
Petri Koho
BPBarbara Pastina
Barbara Pastina
Geologic repositories for spent nuclear fuel use bentonite as a buffer to protect the metallic containers confining the radioactive material. Sulfate-reducing bacteria, which may be present in groundwater, at the bentonite–host rock interface or eventually within the bentonite may produce sulfide, representing a potential threat for the metallic canisters, particularly copper. Bentonites can act as potential sulfide scavengers. Little is yet known, however, regarding the underlying mechanisms, the maximum extent of sulfide consumption, and the potential impacts on bentonite structure under repository conditions. In the current study, concentrated (4–150 mM) sulfide solutions were reacted in batch experiments with six natural Fe-bearing bentonites, with various purified Fe-bearing components of bentonite (a series of purified montmorillonites and three iron (oxyhydr)oxides), and with one synthetic mixture, for up to 1.5 months at pH values ranging from 7 to 13. The solutions were analyzed by colorimetry to determine sulfide and polysulfide concentrations and the solids were analyzed by57Fe Mössbauer spectrometry to determine iron speciation. Important sulfide consumption coupled with a reduction of structural Fe in the clay samples was observed. Not all clay structural Fe was reactive toward sulfide; the proportion of active structural Fe depended on the clay structure and pH. In the presence of excess sulfide in solution regarding Fe in the solid sample, the clay structural Fe was found to be the main reactant while the reaction with iron (oxyhydr)oxides was largely inhibited. Three bentonite groups were distinguished, based on the sulfide oxidation capacity of their main clayey component.