The semi-solid metal (SSM) 5083 aluminum alloy was developed for part manufacturing in the marine shipbuilding industry. This study aimed to optimize the parameters for the friction stir welding process of SSM 5083 aluminum alloy using the Taguchi and analysis of variance (ANOVA) techniques. Our analyses included tensile strength, hardness value, and the microstructure. The results revealed that the optimal parameters obtained for the tensile strength and hardness value in the stir zone (SZ) were A1B1C2 (1000 rpm, 10 mm/min, with a threaded cylindrical tool) with a tensile strength of 235.22 MPa and A2B1C2 (1200 rpm, 10 mm/min, with a threaded cylindrical tool) with a hardness value of 80.64 HV. According to the results obtained by ANOVA, it was found that the welding speed was the most significant process parameter in terms of influencing the tensile strength. Contrarily, no parameter influenced the hardness at a 95% confidence level. The examination using scanning electron microscopy (SEM) and an energy dispersive X-ray spectroscope (EDS) revealed an elongated grain structure and a void defect at the pin tip on the advancing side (AS) in the SZ. The particle distribution was uniform with Al2O3 and small porous SiO2 phases. Moreover, the quantities of C, O, Al, F, and Mg decreased.

1 January 2023 in AIP Conference Proceedings
Verified
Conference Paper
Open access
PDF file
KNkonkrai nakowong
konkrai nakowong
Kittima SillapasaKittima Sillapasa
Kittima Sillapasa
The purpose of this study was to examine the fatigue strength for friction stir welding (FSW) of the semi-solid metal (SSM) 5083 aluminum alloy. The thickness was 6 mm using butt joints. The parameters of the FSW process, the rotational speed of 1200 rpm, welding speed of 10 mm/min, and threaded cylindrical tool profile were tested. The fatigue tests by using the Static and Dynamic Testing Machine, frequency of 20 Hz, the stress ratio of R=−1. Adjust the stroke value to achieve six stress amplitude levels of 0.9, 0.8, 0.7, 0.6, 0.5 and 0.4 mm. A fatigue limit for the FSW and the base metal (BM) of over 3×106 cycles. The results revealed stroke levels at the same level had stress amplitude, and the number of cycles at each level between the FSW and the BM was similar. The endurance limits of the FSW and the BM of 48.501 MPa and 46.569 MPa respectively.