Controlling the microstructure homogeneity is crucial in achieving high quality tantalum (Ta) sputtering targets used in integrated circuit fabrication. Unluckily, traditional rolling easily generates a microstructure gradient along the thickness direction in Ta sheets. The deformation and recrystallization behavior of unidirectional and clock rolled Ta with an 87% strain were therefore systematically compared to investigate whether the change of strain-pass can effectively ameliorate the microstructure gradient along the thickness. Electron backscatter diffraction was used to analyze the misorientation characteristics of the deformed grains. A strong microstructure gradient exists in the unidirectional rolled (UR) sheets. Many microshear bands and well-defined microbands occurred in {111} deformed grains in the UR sheets, especially in the center region, while the grain fragmentation with {111} and {100} orientation in the clock rolled (CR) sheets was more homogenous along the thickness. The kernel average misorientation (KAM) and grain reference orientation deviation-hyper (GROD-Hyper) further confirmed these differences. X-ray line profile analysis (XLPA) indicated that the stored energy distribution was more inhomogeneous in the UR sheets. Schmid factor analysis suggested that the strain path changes due to clock rolling promoted the activation of multiple slip systems in {111} oriented grains. Upon static annealing, homogeneous nucleation combined with a slower grain growth rate resulted in finer and more uniform grain size for the CR sheet. In contrast, a strong recrystallization microstructure-gradient along the thickness formed in the UR sheets, which is attributed to the fact that the higher stored energy and more preferential nucleation sites led to faster recrystallization in the center region, as compared with the surface region. Thus, clock rolling can effectively improve the homogeneity of the through-thickness recrystallization microstructure of Ta sheets.
One hundred and thirty-five degree clock rolling significantly improves the texture homogeneity of tantalum sheets along the thickness, but a distinctly fragmented substructure is formed within {111} (//normal direction (ND)) and {100} (//ND) deformation grains, which is not suitable to obtain a uniform recrystallization microstructure. Thus, effects of different annealing temperatures on the microstructure and texture heterogeneity of tantalum sheets along the thickness were investigated by X-ray diffraction (XRD), electron backscatter diffraction (EBSD) and transmission electron microscopy (TEM). Results show that the texture distribution along θ-fiber and γ-fiber is irregular and many large grains with {111} orientation develop during annealing at high temperature. However, low-temperature annealing can not only weaken the texture intensity in the surface and the center layer but also introduce a more uniform grain size distribution. This result can be attributed to the subgrain-nucleation-dominated recrystallization mechanism induced by recovery at low temperature, and moreover, a considerable decline of recrystallization driving force resulting from the release of stored energy in the deformation matrix.
The microstructure and texture distribution of ultra-high purity Cu-0.1Al alloy target play a key role in the quality of the sputtering film. The Cu-0.1Al alloy sheets were processed by unidirectional (UR) and cross rolling (CR), and X-ray diffraction (XRD), and electron backscatter diffraction (EBSD) technologies were adopted to observe the texture and microstructure evolution. XRD results reveal that the texture types vary greatly in UR and CR due to the change of strain path. As the strain increases to 90%, S texture occupies the most, followed by copper texture in the UR sample, while brass texture dominates the most in the CR sample. Additionally, the orientation density of texture does not increase significantly with the increase of strain but shows a downward trend both in UR and CR modes. EBSD analysis demonstrates that compared with UR, the deformation microstructure in CR is more uniform, and the layer spacing between the deformation bands is smaller, which can reduce the local-region stress concentration. After the completion of recrystallization, the difference in average grain size between the UR and CR-annealed samples is not significant, and the recrystallized grains become much finer with the increase of strain, while more equiaxed grains can be observed in CR-annealed samples.
The evolution of texture and microstructure uniformity in high-purity tantalum (Ta) sheets during 135° warm cross rolling (WCR) was analyzed in detail. X-ray diffraction suggested that relatively uniform ‘ideal’ deformation texture distribution across the thickness could be obtained from WCR, since more potential slip systems could be activated. Electron backscatter diffraction (EBSD) results indicated that the change in strain path in warm rolling could enhance dislocations mobility and increase the probability of dislocations rearrangement and annihilation. Thus, the proportion of low-angle grain boundaries was significantly reduced, and more sub-grain boundaries or sub-grains were formed via WCR. The calculation of geometrically necessary dislocation density based on the strain gradient model supports this result. The analysis of relative Schmid factor combined with the strain contouring map indicated that inhomogeneous orientation-dependent grain subdivision could be effectively weakened, and relatively uniform strain distribution could be formed in the WCR sample. Upon annealing, uniform fine grain size and more randomly oriented grains were obtained in the WCR sample after the completion of recrystallization because of relatively uniform grain subdivision and stored energy distribution.
The texture and the bulk stored energy along the thickness direction were extremely inhomogeneous in the clock-rolled tantalum sheets with 70% reduction. Therefore, the effects of different annealing temperatures on the microstructure and texture distribution of tantalum plates through the thickness were investigated by X-ray diffraction (XRD) and electron backscatter diffraction (EBSD). The results showed that the occurrence of strong {111} recrystallization texture in the center layer can be attributed to the subgrains nucleation mechanism when annealed at the low temperature. Many subgrains with {111} orientation appeared in the center layer, due to its high stored energy and preferential nucleation sites of the {111} deformed matrix, and rapidly grew into the effective nucleus, resulting in the large {111} grain size and strong {111} texture after complete recrystallization. Contrarily, at the high temperature, high-angle grain boundaries had sufficient driving force to generate migration, due to the lack of recovery, and the growth time of recrystallized nucleus was much shorter, contributing to relatively uniform recrystallization microstructure and texture distribution along the thickness.