Orbital pipe welding was often used to manufacture piping systems. In orbital pipe welding, a major challenge is the welding torch’s position during the welding process, so that additional methods are needed to overcome these challenges. This paper discusses the influence of welding sequence and welding current on distortion, mechanical properties and metallurgical observations in orbital pipe welding with SS 316L pipe square butt joints. The variation of the orbital pipe welding parameters used is welding current and welding sequence. The welding current used is 100 A, 110 A, and 120 A, while the welding sequence used is one sequence, two sequences, three sequences, and four sequences. The welding results will be analyzed from distortion measurement, mechanical properties test and metallurgical observations. Distortion measurements are made on the pipe before welding and after welding. Testing of mechanical properties includes tensile tests and microhardness tests, while metallurgical observations include macrostructure and microstructural observations. The results show that maximum axial distortion, transverse distortion, ovality, and taper occurred at a welding current of 120 A with four sequences of 445 µm, 300 µm, 195 µm, and 275 µm, respectively. The decrease in ultimate tensile strength is 51 % compared to the base metal’s ultimate tensile strength. Horizontal and vertical microhardness tests show that welding with one sequence produces the greatest microhardness value, but there is a decrease in the microhardness value using welding with two to four sequences. Orbital pipe welding results in different depths of penetration at each pipe position. The largest and smallest depth of penetration was 4.11 mm and 1.60 mm, respectively
30 March 2020 in International Journal of Automotive and Mechanical Engineering
In this research, the effect of pulse currents on the weld geometry and angular distortion in pulsed GTAW (PGTAW) process in 3 mm thick SS-304 autogenous butt weld joint was investigated. Welding method uses pulse current and continuous current. The mean current and welding speed were kept constant with the peak current and base current were varied. During pulsed GTAW process, the arc condition was captured directly using a charge-coupled device (CCD) camera. Weld geometry was carried out using a digital microscope. Distortion was measured using Coordinate Measuring Machine (CMM). The results show that the peak current and base current have an influence on weld geometry and angular distortion. The weld geometry on pulsed GTAW was produced wider of weld bead width than continuous GTAW. However, angular distortion on continuous GTAW was higher than pulsed GTAW. Pulsed GTAW can widen the weld bead by 0.57% - 25.09%, but can reduce distortion by 15.15%-88.17%. As compared with weld geometry to the continuous GTAW, the widest result occurs at peak current 212A and base current 40A. The smallest of distortion on pulsed GTAW was achieved at peak current 138A and base current 80A.
In this study, the GMAW parameters for welding of A36 mild steel have been investigated to get the minimum of distortion. The type of welded joint used was square groove T-joint fillet weld with filler wire ER70S-6. The welding current and the welding speed were selected as input parameters while the response used was distortion (longitudinal bending distortion and angular distortion). Taguchi method was used to determine optimal welding parameters which the minimum distortion. Design of experiment was set two factors with three level in each factor and three replication, so the L9 Taguchi’s orthogonal array was applied. The minimum conditions were determined using S/N ratio with a quality character of smaller is better (SB). In addition, to determine the significance of the welding parameters used ANOVA. The results show that the welding current of 170 A and the welding speed of 4.0 mm/s were obtained as the minimum of longitudinal bending distortion and angular distortion. Based on analysis of variance, the welding current was a parameter that greatly affects the longitudinal bending distortion with the percentage contribution of 64.36% while angular distortion was strongly influenced by welding speed parameter with the percentage contribution of 53.38%.
1 November 2019 in IOP Conference Series: Materials Science and Engineering
In this study, the effect of welding current and welding speed on the weld geometry and distortion in TIG welding process was investigated. The material used in this experiment is A36 mild steel pipe. The dimensions of specimen were 114.3 mm of outer diameter and 6 mm of thickness. The wire feeder used was ER70-S 6 with a V-groove joint as a type welding joint. The welding parameters varied were the welding current and welding speed. Welding results will be tested for weld geometry (outer bead width) and distortion after the welding process. The weld geometry was measured using Digital Microscope and the distortion was measured using outside micrometers before and after the welding process. The results show that increasing the welding current can widen the weld bead and increase distortion. While increasing the speed has little effect on the weld bead and distortion. Welding parameters with a welding current of 170 A and a welding speed of 0.9 mm/s produces the widest outer bead and the biggest tapers and distortion. In addition, the results of tapers and distortion in the axial direction were greater than the transverse direction of the pipe.
1 January 2020 in IOP Conference Series: Materials Science and Engineering
In the present study, the PC-GTAW orbital welding parameters of AISI 304L stainless steel pipe have been optimized by using ANOVA and Taguchi method. The welding method uses Pulsatile Current-GTAW without added material (autogenous). Peak currents were varied in this study and had the same average current of 100 ± 0.5 amperes. The Taguchi method was applied to search for OBW, DoP and UTS that are optimal and L16 Taguchi’s orthogonal array with two factors, four levels and two replications. S/N ratio with a quality character of larger is better (LB) was used to find the maximum value. The results show that raising the peak current would widen the OBW and deepen the DoP but reduce UTS. The 35-C parameter was the optimal parameter to produce OBW and DoP while the 100-C parameter was the optimal parameter to produce maximum UTS.
20 January 2025 in Journal of Advanced Research in Fluid Mechanics and Thermal Sciences
Intense braking can cause heat accumulation that can reduce the braking system’s efficiency and damage the braking system components due to changes in material structure. The high temperature in the braking system of heavy vehicles requires an air-cooling system that produces high-pressure air. This study compares the cooling process results between natural air and forced air. CFD modeling was chosen as the method to simulate the cooling process of bus drum brakes. The CFD method works by involving a network of elements in a system called a mesh. In CFD, the mesh is a component that focuses on dividing the fluid domain into small elements to analyze fluid flow, heat transfer, and dynamic phenomena. Using a cooling process, the brake system temperature gradually decreased as the wind speed increased. The examination proved that natural air could reach the highest temperature of 168.73 °C and the lowest temperature of 63.01 °C. Meanwhile, forced air could reach the highest temperature of 73.8 °C and the lowest temperature of 30.73 °C. Statistical models and machine learning were carried out to predict the accuracy of simulation from SOLIDWORKS. The values of average temperature after the cooling process are examined by employing the Gradient Boosting algorithm with the highest accuracy of prediction (R2) value of 0.999895 in natural conditions and 0.999822 in forced conditions. Overall, forced air shows better temperature reduction than natural air. By lowering the operating temperature, drum brake systems can extend their lifespan.