Very high temperature creep properties of twelve different Ni-based single crystal superalloys have been investigated at 1250 °C and under different initial applied stresses. The creep strength at this temperature is mainly controlled by the remaining γ′ volume fraction. Other parameters such as the γ′ precipitate after microstructure evolution and the γ/γ′ lattice parameter mismatch seem to affect the creep strength to a lesser degree in these conditions. The Norton Law creep exponent lies in the range 6–9 for most of the alloys studied, suggesting that dislocation glide and climb are the rate limiting deformation mechanisms. Damage mechanisms in these extreme conditions comprise creep strain accumulation leading to pronounced necking and to recrystallization in the most severely deformed sections of the specimens.
In this study, resistivity measurements are made during continuous heating and cooling on four different Ni-based superalloys of different grain structures and with different phases (i.e.,γ′ and carbide). The results are directly compared with differential scanning calorimetry (DSC) profiles to identify the material’s resistivity response. The resistivity measurements have been performed using an electro-thermal mechanical testing (ETMT) system having a capability of heating and cooling a sample at a rate of up to 100 K/s by Joule heating, which is not possible with standard heating methods used in previousin-situmicrostructure analysis approaches. By comparing different precipitate variations and thermal histories,γ′ volume fraction and precipitate number density are found to be the most important factors determining the resistivity of the materials.In-situresistivity measurement was applied to several case studies to show that it can provide microstructural information in complex high temperature experiments.
This is a first report on profilometry‐based indentation plastometry (PIP) at high temperature (HT), covering both thermal characterization and issues for obtaining stress–strain curves. The heating system has a relatively low thermal inertia, reaching 800 °C within about 10 min, while both indentation (≈20 s) and cooling (≈20 min) are also quick. This capability is useful in terms of limiting exposure of the sample to prolonged periods at HT, and hence avoiding the formation of thick oxide layers (which can affect indent profiles and hence inferred stress–strain curves). There is good general consistency between stress–strain curves obtained via HT‐PIP and those from tensile testing. However, the possibility of creep (time‐dependent deformation) affecting the outcomes (of both types of test), particularly at higher temperatures, should be borne in mind. Creep has a characteristic effect on tensile curves, which can often be confirmed and investigated by changing the imposed strain rate. It can also be revealed by carrying out the HT‐PIP testing with different penetration velocities or by monitoring the shape of the load–displacement plot.