The enzymatic degradation of poly(lactic acid) was catalyzed with Proteinase K and the effect of various factors on the rate of degradation was analyzed quantitatively with the help of appropriate kinetic models. The Michaelis-Menten model was modified for the purpose by considering the heterogeneous nature of the reaction and the denaturation of the enzyme. The results proved that Proteinase K degrades the polymer very efficiently. The rate of degradation increases considerably up to 0.1 mg/ml enzyme concentration, but remains constant at larger values. Temperature has an optimum at around 50 °C that is somewhat higher than the 37 °C extensively used in the literature as the most advantageous temperature. If degradation occurs in the same medium throughout the process, the formation of lactic acid results in the rapid decrease of pH and finally in the denaturation of the enzyme. The dropping of pH below 5 slows down and finally stops degradation completely. The daily change of the medium results in degradation with a constant rate and the entire amount of the polymer can be decomposed mainly into monomer or smaller oligomer fragments. Degradation rate decreases slightly with increasing molecular weight and increasing d-lactide content. The use of appropriate kinetic models allows quantitative analysis and the prediction of the rate of enzymatic degradation of PLA.
Purpose: Electrospun PLA fiber devices were investigated in the form of fiber mats and disks. Metronidazole was used as an active agent; its concentration was 12.2 and 25.7 wt% in the devices. Methods: The structure was studied by X-ray diffraction and scanning electron microscopy, drug release by dissolution measurements, while the antimicrobial efficiency was tested on five bacterial strains. Results: The XRD study showed that the polymer was partially crystalline in both devices, but a part of metronidazole precipitated and was in the form of crystals among and within the fibers. Liquid penetration and dissolution were different in the two devices, they were faster in disks and slower in fiber mats, due to the morphology of the device and the action of capillary forces. Disks released the drug much faster than fiber mats. Although the release study indicated fast drug dissolution, the concentration achieved a plateau value in 24 hrs for the disks; the inhibition effect lasted much longer, 13 days for bacteria sensitive to metronidazole. The longer inhibition period could be explained by the slower diffusion of metronidazole located inside the fibers of the device. Conclusion: The results suggest that the devices may be effective in the treatment of periodontitis.
PLA fibers containing metronidazole as the active component were produced by electrospinning from a solvent mixture of dichloromethane (DCM) and dimethyl sulfoxide (DMSO). The DMSO content of the spinning solution changed between 0 and 25 vol% in 5 vol% steps. The fibers were dried at different temperatures, and processes taking place during fiber production and drying were followed by thermogravimetric analysis and differential scanning calorimetry. The morphology and structure of the fibers were studied by microscopy and X-ray diffraction. The mechanical properties of fiber mats and the release of the drug were also determined as a function of processing and drying parameters. The results showed that several processes take place during the production and subsequent handling of the fibers including the evaporation of the solvent (DMSO), the crystallization of the polymer, the changing of composition, phase separation and the consequent partitioning of the drug. The crystalline structure of the fibers changes considerably during drying which determines their mechanical properties. The rate of evaporation and crystallization is in the same order of magnitude. The rate of both processes increases considerably with temperature, but does not depend strongly on the amount of DMSO in the spinning solution. Both the amount of the drug released and the rate of release cover a wide range depending on the parameters of the preparation technology. The large range of mechanical and functional properties obtained allows the control of the kinetics of drug release to some extent.
Electrospun fibers containing levocetirizine, a BCS III drug, were prepared from three water-soluble polymers, hydroxypropyl methylcellulose (HPMC), polyvinylpyrrolidone (PVP) and polyvinyl alcohol (PVA). Fiber-spinning technology was optimized for each polymer separately. The polymers contained 10 wt% of the active component. An amorphous drug was homogeneously distributed within the fibers. The solubility of the drug in the polymers used was limited, with a maximum of 2.0 wt%, but it was very large in most of the solvents used for fiber spinning and in the dissolution media. The thickness of the fibers was uniform and the presence of the drug basically did not influence it at all. The fiber diameters were in the same range, although somewhat thinner fibers could be prepared from PVA than from the other two polymers. The results showed that the drug was amorphous in the fibers. Most of the drug was located within the fibers, probably as a separate phase; the encapsulation efficiency proved to be 80–90%. The kinetics of the drug release were evaluated quantitatively by the Noyes–Whitney model. The released drug was approximately the same for all the polymers under all conditions (pH), and it changed somewhere between 80 and 100%. The release rate depended both on the type of polymer and pH and varied between 0.1 and 0.9 min−1. Consequently, the selection of the carrier polymer allowed for the adjustment of the release rate according to the requirements, thus justifying the use of electrospun fibers as carrier materials for levocetirizine.