Solid solutions in the Ba(Pb1−xSrx)O3−z system were prepared by aliovalent substitution of Pb4+ by Sr2+ ions to investigate the effect of cation stoichiometry on thermal and electrical properties as x was varied between 0 and 0.4, in the temperature range 300–523 K. The starting compound, barium plumbate (BaPbO3), has a perovskite structure and is known to exhibit metallic conductivity due to an overlap of the O2p nonbonding and the Pb–O spσ antibonding band, which is partially filled by the available electrons. The large difference in the ionic radii between the Pb4+ and Sr2+ ions introduces significant strain into the (Pb/Sr)O6 octahedra of the perovskite structure. Additionally, charged defects are created on account of the different oxidation states of the Pb4+ and Sr2+ ions. Evidence of a metal to insulator transition (MIT) of the Mott–Hubbard type has been observed at a critical concentration of Sr2+ ions.
We have investigated the influence of the relative proportions of glass formers in a series of lithium alumino-borosilicate glasses with respect to electrical conductivity (σ) and glass transition temperature (Tg) as functions of glass structure, as determined using Raman spectroscopy. The ternary lithium alumino-borate glass exhibits the highest σ and lowest Tg among all the compositions of the glass series, 30Li2O•3Al2O3• (67−x) B2O3•xSiO2. However, as B2O3 is replaced by SiO2, a shallow minimum in σ, as well as a shallow maximum in Tg, are observed near x = 27, where the Raman spectra indicate that isolated diborate/tetraborate/orthoborate groups are being progressively replaced by danburite/reedmergnerite-like borosilicate network units. Overall, as the glasses become silica-rich, σ is minimized, while Tg is maximized. In general, these findings show correlations among Tg (sensitive to network polymerization), σ (proportional to ionic mobility), and the different borate and silicate glass structural units as determined using Raman spectroscopy.
Crystal structures, microtopography, morphologies, elemental compositions, and ionic conductivity have been investigated for Li
5-
x La 3 (Nb,Ta)O
12-
y using X-ray diffraction (XRD), field-emission analytical scanning and transmission electron microscopies (S/TEM), and electrochemical impedance spectroscopy. Using Rietveld refinements with powder XRD patterns, we determined that the number of Li atoms in the formula is less than 5 and that Li
5-
x La 3 (NbTa)O
12-
y crystallizes in the cubic garnet structure with a space group Ia- 3 d . Sintering at varying temperatures (750–1000 °C) for 5 h in an ambient atmosphere produced distinct outcomes. Rietveld refinements disclosed that the sample sintered at 1000 °C (Li 3.43(2) La 3 Nb 1.07(2) Ta 0.93(2) O
12-
y , a = 12.8361(7) Å, V = 2114.96(3) Å3) exhibited the highest ionic conductivity, while the 850 °C sample had the lowest conductivity, characterized by lower Li concentration and impurity phases (Li(Nb,Ta) 3 O 88 , Li 2 CO 3 ). Analyses, including XRD and electron microscopy, confirmed the 1000 °C sample as a relatively phase pure with enhanced Li content (Li/La = 1.2), larger grains (15 μm), and uniform crystallinity. The 1000 °C sample introduced additional partially filled Li3 (96 h ) sites, promoting Li migration, and enhancing ionic conductivity. The resulting XRD pattern at 1000 °C has been submitted to the Powder Diffraction File as a reference.
This study presents the electrical and optical properties of 35P2O5–xV2O5–(65–x) Sb2O3 glasses for 0 ≤ x ≤ 65 mol%. The direct current (DC) resistivity was measured by the Van der Pauw method and optical absorption spectra were taken in the Ultraviolet–Visible-Near-Infrared (UV–VIS–NIR) range. Electrical transport is attributed to simultaneous hopping of small polarons (SPs) between V4+ and V5+ (vanadium ion) sites and small bipolarons (SBPs) between the Sb3+ and Sb5+ (antimony ion) sites. The resistivity exhibits a non-linear dependence on the ionic fraction of vanadium (nv), whereas the resistivity exhibits a minimum in the composition range 0 ≤ nV ≤ 0.3, and a resistivity maximum was observed in the range 0.3 ≤ nV ≤ 0.5. On further increasing nv, the resistivity exhibits a monotonic decline. In the composition range 0 ≤ nV ≤ 0.3, where the hopping distance between V ions decreases, while that between the Sb ions increases, the resistivity minimum has been shown to be the consequence of decreasing tunneling distance of SPs between the V4+ and V5+ ion sites. In the composition range 0.3 ≤ nV ≤ 0.5, the resistivity, activation energy for DC conduction, glass transition temperature, and density exhibit their respective maxima even though the separation between the V4+ and V5+ sites continues to decrease. This feature is explained by enhanced localization of electrons on account of increased disorder (entropy) among the SPs and SBPs, like that of Anderson localization. This argument is further supported by a shift in the polaronic optical absorption bands associated with the SPs and SBPs toward higher energies. The transport behavior of all the glasses except the x = 0 composition has been explained by adiabatic transport, principally, by the SPs on V ions while the Sb ions contribute little to the total transport process. The results provide a clear relation between composition, polaron/bipolaron contributions, and conduction in these glasses.
We present a fresh perspective on the mixed halogen-ion effect (MHE) in lead silicate glasses containing a mixture of halogen ions with a correlative study of optical spectroscopy and halogen ion transport. PbO was partially substituted by either PbCl2 or PbF2 in the ternary glass system: (65 − x) − x(PbF2 or PbCl2)-35SiO2 (where 0 ≤ x ≤ 20 mol%) and by a mixture of PbF2 and PbCl2 in the quaternary glass series: 45PbO − xPbF2 − (20 − x)PbCl2–35SiO2 (where 0 ≤ x ≤ 20 mol%). A suite of improved characterization techniques, including 4-probe van der Pauw resistivity measurements, optical absorption spectroscopy, differential thermal analysis, etc., was employed to correlate composition with physical properties. Replacing PbO with small quantities of PbF2 or PbCl2 in binary 65PbO-35SiO2 glass resulted in a dramatic increase in conductivity by 3–4 orders of magnitude, confirming a shift from Pb2+-mediated to halide ion-mediated conduction and, within the mixed-halogen series, a profound MHE was observed. Contrary to previously reported data, the activation energy for conduction and the resistivity both exhibited maxima at the mixed halogen-ion ratio, MHR = (F/(F + Cl), of 0.5. The glass transition temperature (Tg) exhibited a non-monotonic trend, peaking at 506 °C for the MHR = 0.5 composition. Optical absorption measurements have revealed that the MHR = 0.5 glass has the broadest absorption edge and also exhibits certain features in the near IR region of the Urbach tail, which are suggestive of maximum electronic disorder.