A simple heat treatment method was used to optimize the three-dimensional network structure of the hydrophobic aerogel, and during the heat treatment process at 200–1000 °C, the thermal conductivity of the aerogel reached the lowest to 0.02240 W/m·K between 250 °C and 300 °C, which was mainly due to the optimization of microstructure and pyrolysis of surface groups. Further Fluent heat-transfer simulation also confirmed the above results. Synchrotron vacuum ultraviolet photoionization mass spectrometry (SVUV-PIMS) was used to finely measure the pyrolysis process of aerogels, and the pyrolysis process of aerogel was divided into four stages. (I) Until 419 °C, as the temperature continued to rise, surface methyl groups were oxidized to form hydroxyl. (II) As the temperature reached to 232 °C, the oxidation proceeded. In addition, inside the aerogel, because of lacking oxygen, the reaction produced CH4 and C–Si bonds would form. (III) After 283 °C, Si–OH groups began to condense to form Si–O–Si, which optimized the three-dimensional network structures to be beneficial to improve the thermal insulation performance of silica aerogel. (IV) When it reached 547 °C, the chemical reaction was terminated, and all the primary particles gradually fused into secondary particles and sintered to form clusters.
Polyimide aerogels were prepared using low-cost polymers with different structure capped polyamide oligomers serving as cross-linking agents. To investigate the effects of the anhydride density on cross-linker chain units and side groups of cross-linkers on their properties and microstructures, two kinds of polymers from maleic anhydride, endic anhydride, and styrene were prepared by simple radical polymerization. The polyimide aerogels exhibit densities as low as 0.087 g cm−3 and specific surface areas as high as 456 m2 g−1. And the maximum modulus of the aerogel is up to 21.3 MPa. These cross-linkers are alternatives to expensive small molecule cross-linkers, therefore reducing the cost of PI aerogels.
SiO2 aerogels have garnered significant attention for thermal insulation applications due to their exceptional hydrophobicity and thermal resistance. However, the organic functional groups enabling hydrophobicity introduce flammability concerns, limiting their safe implementation in high-temperature environments. This study presents a novel TiO2 doping strategy (SA/TiO2) that simultaneously enhances thermal safety while preserving the material’s intrinsic advantages. The optimized SA/TiO2 composite demonstrates remarkable fire resistance, achieving a 44% reduction in gross calorific value (GCV) and a 25.4% decrease in total heat release (THR) compared to conventional aerogels. Thermogravimetric analysis reveals substantial thermal stability improvements, with TiO2 incorporation elevating the initial and peak decomposition temperatures by 207 °C and 167 °C, respectively. When integrated into fiber-reinforced SiO2 aerogel composites, the 10% TiO2-doped formulation achieves an ultra-low GCV of 2.75 MJ/kg while maintaining superior insulation performance (~18 mW/m·K). Notably, the composite demonstrates exceptional high-temperature stability, retaining minimal thermal conductivity of 25.5 mW/m·K at 600 °C. The titanium dioxide phase effectively attenuates thermal radiation transmission while preserving the matrix’s nanoporous architecture, thereby synergistically enhancing both fire safety and thermal insulation capabilities in demanding operational environments.
1 September 2004 in Zeitschrift für angewandte Mathematik und Physik
Polyimide (PI) aerogels were prepared using self-designed silicone polymer cross-linkers with multi-amino from low-cost silane coupling agents to replace conventional small-molecule cross-linkers. The long-chain structure of silicone polymers provides more crosslinking points than small-molecule cross-linkers, thus improving the mechanical properties of polyimide. To investigate the effects of amino content and degree of polymerization on the properties of silicone polymers, the different silicone polymers and their cross-linked PI aerogels were prepared. The obtained PI aerogels exhibit densities as low as 0.106 g/cm3 and specific surface areas as high as 314 m2/g, and the maximum Young’s modulus of aerogel is up to 20.9 MPa when using (T-20) as cross-linkers. The cross-linkers were an alternative to expensive small molecule cross-linkers, which can improve the mechanical properties and reduce the cost of PI aerogels.