Katrapally Vijaya Kumar

Prof. Dr. Katrapally Vijaya Kumar


Research Focus & Metrics

Academic Career Length

11Years (2016-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
23 March 2016 in Physics Research International
Verified
Journal Article
Open access
PDF file
VSV. Srinivas
V. Srinivas
ARA. T. Raghavender
A. T. Raghavender
KKKatrapally Vijaya Kumar
Katrapally Vijaya Kumar
Nanocrystalline Bi1-xMnxFeO3 (0≤x≤0.3) materials were synthesized using sol-gel technique. The structural and magnetic properties were investigated in detail. Rietveld analysis from XRD revealed the structural formation of BiFeO3. As the Mn doping concentration was increased, the structure of BiFeO3 changed from rhombohedral to tetragonal. All the M-H loops showed the ferromagnetic behavior in the prepared samples. Magnetization was observed to enhance as the Mn doping concentration was increased. The enhanced magnetization may be due to the collapse of the space modulated spin structure as observed from the structural changes.

9 September 2022 in Phase Transitions
Verified
Journal Article
Closed access
KKKatrapally Vijaya Kumar
Katrapally Vijaya Kumar
SBSara Durga Bhavani
Sara Durga Bhavani
Erbium-doped zinc ferrite nanoparticles (ZnFe1.9Er0.1O4) were prepared by the sol–gel auto-combustion method. In order to study the impact of calcination temperature, the prepared powder was divided into four parts and calcinated at 700, 900, 1100 and 1300°C. XRD confirmed the formation of a spinel structure with a single phase and Fd3m space group. Crystallite size increased from 19.45 to 30.22 nm with the increase in calcination temperature. SEM images showed agglomerated flakes having voids and pores on the surface. The average grain size increased from 157.76 to 237 nm with the increase in calcination temperature. FTIR showed two fundamental absorption bands related to octahedral and tetrahedral sites along with other three absorption bands in the frequency range 400–4000 cm−1. The optical energy bandgap was increased from 3.8166 to 4.2779 eV with the increase of calcination temperature. Hence, it is concluded that the optical energy bandgap can be tuned with the calcination temperature.

4 September 2023 in East European Journal of Physics
Verified
Journal Article
Open access
PDF file
KKKatrapally Vijaya Kumar
Katrapally Vijaya Kumar
SBSara Durga Bhavani
Sara Durga Bhavani
Nickel aluminate (NiAl2O4) nanoparticles were synthesized using sol-gel method with auto-combustion. The prepared nanoparticles were made into four parts and calcinated at 700, 900, 1100 and 13000C and taken up for the present study. The taken-up nanoparticles were characterized using powder X-Ray Diffraction (XRD), Scanning Electron Microscopy (SEM), Energy Dispersion X-Ray Spectroscopy (EDS), Fourier Transform and Infrared (FT-IR) spectroscopy and UV-Vis spectroscopy techniques. The X-ray diffraction patterns confirmed the spinel structure and Fd3m space group. Scherrer formula was used to calculate the crystallite size and found in the range 5.78 to 20.55 nm whereas the lattice parameter was found in the range of 8.039 to 8.342 Å. The average grain size was found in the range 142.80 to 187.37 nm whereas interplanar spacing was found in the range of 2.100 to 2.479 Å. The FTIR spectroscopy showed six absorption bands in the range 400 to 3450 cm-1 and confirmed the spinel structure. The optical band gap (Eg) was decreased with calcination temperature and found in the range 4.2129-4.3115eV.

1 January 2022 in Science of Sintering
Verified
Journal Article
Open access
PDF file
KKKatrapally Vijaya Kumar
Katrapally Vijaya Kumar
SBSara Durga Bhavani
Sara Durga Bhavani
Nickel chromite nanoparticles were prepared by sol-gel auto combustion method followed by calcination at different temperatures, 700, 900, 1100 and 1300oC for 8h. The prepared nanoparticles were characterized by XRD, SEM, EDS, FTIR and UV-Vis spectroscopy. From the XRD patterns, the Miller indices (hkl) were identified for all the prominent peaks for all the samples, it was clear that the compound crystallized according to spinel structure with a space group of Fd3m. SEM images showed non-uniform agglomerated fragments having a lot of voids and pores. UsingScherrer method, the crystallite size was calculated and found gradually increasing trend with the calcination temperature from 13.73 to 22.33 nm, where as the average grain size was increased from 140.00 to 163.46 nm with calcination temperature. FTIR spectra showed six fundamental absorption bands in the range 500 to 3470 cm-1, whereas the two absorption bands in the range 500-625 cm-1 confirmed the bonding vibrations of metal-oxygen bonds situated at octahedral and tetrahedral sites. UV-Vis spectroscopy was carried out in the wavelength range 200-800 nm and the optical band gap (Eg) was observed in the range 4.2129-4.3115 eV.

29 July 2024 in Journal of Materials Science: Materials in Electronics
Verified
Journal Article
Closed access
PDF file
SBSara Durga Bhavani
Sara Durga Bhavani
BRB. Purna Chandra Rao
B. Purna Chandra Rao
KKKatrapally Vijaya Kumar
Katrapally Vijaya Kumar
NKN. Hari Kumar
N. Hari Kumar
MSMadireddy Buchi Suresh
Madireddy Buchi Suresh

1 January 2016 in Processing and Application of Ceramics
Verified
Journal Article
Open access
PDF file
KSKumar Naraavula Suresh
Kumar Naraavula Suresh
KKKatrapally Vijaya Kumar
Katrapally Vijaya Kumar
Bismuth doped nano zinc ferrite particles having the general formula ZnFe2-xBixO4 (x = 0.00, 0.05, 0.10, 0.15, 0.20 and 0.25) were synthesized by sol-gel combustion method. The effect of bismuth doping on structural properties were investigated. The X-ray diffraction (XRD) spectra confirm the single phase cubic spinel structure. The average crystallite sizes of all the samples were determined by Debye-Scherrer equation and are in the range 16-20 nm. The lattice parameter increases with the increase of bismuth ion concentration. This is due to the larger ionic radius of Bi3+ ions substituting smaller Fe3+ ions at octahedral sites (B-sites). The surface morphology of all compounds was studied by scanning electron microscope (SEM). The microstructure analysis and the particle size were examined by transmission electron microscope (TEM). The compositional stoichiometry of these samples was verified by energy dispersive spectroscopy (EDS) analysis.