One of the most important characteristics for the development of biomaterials based on hyaluronic acid (HA) and its chemically modified derivatives is resistance to hyaluronidases (HA-ase), which are responsible for the degradation of HA macromolecules. In this work, samples of phosphorylated (HA-P) low- and high-molecular-weight HA (43 kDa and 0.5–0.7 MDa) were obtained by conventional stirring of HA/P2O5 mixtures at different molar ratios (1:0.2, 1:0.5, 1:1, and 1:2) and exposed to bovine testicular HA-ase (60 or 600 ME/mL, [HA] = 4 mg/mL of citrate buffer, pH 6.3, 16–18 h). It was found that the biodegradability of the HA-P samples obtained at the ratio of 1:0.2, 1: 0.5, and 1:1 was at the level of native HA or higher. Only samples obtained at a HA/P2O5 ratio of 1:2 showed resistance to HA-ase; their biodegradability was 13–54% lower compared to that of native HA.
Chemical phosphorylation of hyaluronic acid (HA) remains an unresolved problem for the chemistry of this unique polysaccharide, since convenient phosphorylating reagents are not reactive enough to obtain HA phosphates (HA-P) with a satisfactory degree of esterification of hydroxyl groups. The synthesis of phosphates of low-molecular-weight (43 kDa) and high-molecular-weight (0.5–0.7 MDa) HA was undertaken using such reagents as sodium trimetaphosphate Na3P3O9, H3PO4, NaH2PO4/Na2HPO4, and anhydride P2O5. Solid-phase HA esterification with P2O5 was found to be the most convenient and efficient method. The HA-P samples were characterized by XRF and NMR spectroscopy (31P and 1H-31P) and contained, depending on the HA/P2O5 ratio, 0.30–6.25% P wt., in the form of disubstituted mono-, di-, and polyphosphates.