Zhong Sheng Li

Zhong Sheng Li


Research Focus & Metrics

Academic Career Length

6Years (2021-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
17 November 2021 in Coatings
Verified
Journal Article
Open access
PDF file
MZMin Zhang
Min Zhang
DPDong Peng
Dong Peng
FPFeifei Peng
Feifei Peng
AHAnwei Huang
Anwei Huang
KSKaiqiang Song
Kaiqiang Song
ZLZhong Sheng Li
Zhong Sheng Li
The Al coatings were electrodeposited on the Cu substrate from AlCl3-EMIC ionic liquid (AlCl3:EMIC = 2:1 molar ratio) containing three cyanopyridine additives with different positions of the substituent group on the pyridine ring, which were 2-cyanopyridine, 3-cyanopyridine, and 4-cyanopyridine. The effects of cyanopyridine additives on the deposition potential, morphology, brightness, and corrosion properties of Al coatings were investigated. It was considered that the deposition potential of Al shifted to more negative overpotentials, the quality of Al coatings was promoted, and the corrosion property was improved by the cyanopyridine additives to a varying degree. Especially in the presence of 4-cyanopyridine, the flattest mirror bright Al coating was obtained, which had the smallest homogeneous nanocrystal grain size and strongest Al (200) crystallographic orientation. The average roughness Ra value was as low as 31 nm compared to that in the absence of cyanopyridine additives, which was 417 nm. Furthermore, the corrosion current density of the bright Al coating was three orders of magnitude lower than the rough Al coating, which resulted from the dense nanocrystal structure.

19 October 2021 in Materials
Verified
Journal Article
Open access
PDF file
DPDong Peng
Dong Peng
DCDa Long Cong
Da Long Cong
KSKaiqiang Song
Kaiqiang Song
XDXingxing Ding
Xingxing Ding
XWXuan Wang
Xuan Wang
ZLZhong Sheng Li
Zhong Sheng Li
The effects of three pyridine derivative additives, 4-hydroxypyridine, 4-picolinic acid, and 4-cyanopyridine, on Al-Mn coatings were investigated in 1-ethyl-3-methylimidazolium chloride-AlCl3-MnCl2 (EMIC-AlCl3-MnCl2) ionic liquids. The smooth mirror-like bright Al-Mn coatings were obtained only in the EMIC-AlCl3-MnCl2 ionic liquids containing 4-cyanopyridine, while the matte Al-Mn coatings were electrodeposited from EMIC-AlCl3-MnCl2 without additives or containing either 4-hydroxypyridine or 4-picolinic acid. The scanning electron microscope and X-ray diffraction showed that the bright Al-Mn coatings consisted of nanocrystals and had a strong (200) preferential orientation, while the particle size of matte Al-Mn coatings were within the micron range. The brightening mechanism of 4-cyanopyridine is due to it being adsorbed onto the cathode to produce the combined effect of (1) generating an overpotential to promote Al-Mn nucleation; (2) inhibiting the growth of the deposited nuclei and enabling them grow preferentially, making the coating composed of nanocrystals and with a smooth surface. The brightening effect of 4-cyanopyridine on the Al-Mn coatings was far better than that of the 4-hydroxypyridine and the 4-picolinic acid. In addition, the bright Al-Mn coating was prepared in a bath with 6 mmol·L−1 4-cyanopyridine and displayed superior corrosion resistance relative to the matte coatings, which could be attributed to its unique nanocrystalline structure that increased the number of grain boundaries and accelerated the formation of the protective layer of the corrosion products.

22 October 2022 in Coatings
Verified
Journal Article
Open access
PDF file
ZLZhong Sheng Li
Zhong Sheng Li
HWHulin Wu
Hulin Wu
YBYixin Bai
Yixin Bai
DCDa Long Cong
Da Long Cong
AHAnwei Huang
Anwei Huang
DPDong Peng
Dong Peng
In order to explore the corrosion damage behavior of plasma-sprayed NiCoCrAlY/magnesia-stabilized zirconia (18~22 wt.% MgO-ZrO2, MSZ) thermal barrier and anti-ablation coatings in a salt spray environment, a series of neutral salt spray (NSS) tests for 96 h (N-2), 192 h (N-4) and 288 h (N-6) were carried out on the coatings. The microstructures, composition distributions, potentiodynamic polarization curves, bonding strengths and anti-ablation properties of the coatings before and after the NSS tests were characterized. The results show that, with the increase in salt spray time, the expansion and overflow of corrosion products (FexOy) led to more defects forming inside the coating; the porosity of the top coat (TC) of N-6 increased to 15.2% in comparison to that of the blank control sample (N-0), which was 8.5%. According to the potentiodynamic polarization curves, accelerated corrosion occurred in the coating samples after the salt spray time reached 192 h, and the corrosion current density rapidly surged from 2.2 × 10−8 A·cm−2 (N-4) to 2.2 × 10−5 A·cm−2 (N-6). Similar degradation tends could be found in the bonding strengths and mass ablation rates of the coatings due to the accumulation of loose corrosion products on the substrate, which affected the bonding states of the coatings and promoted their spalling under an oxyacetylene flame (OAF). As a result, the maximum service life of the NiCoCrAlY/MSZ coatings in the neutral salt spray environment was about 192 h. This work is instructive for studying the environmental adaptability of metal/ceramic double-layer coatings.

25 November 2022 in Metals
Verified
Journal Article
Open access
PDF file
ZLZhong Sheng Li
Zhong Sheng Li
ZLZhengtao Liu
Zhengtao Liu
DCDajun Chen
Dajun Chen
FMFei Mo
Fei Mo
YFYangfan Fu
Yangfan Fu
DCDa Long Cong
Da Long Cong
In this paper, 6061-T6 aluminum alloy and 30CrMnSiA steel are bonded by inertia radial friction welding (IRFW). The formation mechanism of the aluminum/steel friction welded joints and the effect of the welding parameters on the mechanical properties are investigated through the microstructure, microzone composition, and mechanical property analysis. The results show that no visible intermetallic compound layers (IMCs) are detected on the aluminum/steel welding interface, which may be due to Si element aggregating in the welding interface and then forming a Al−Fe−Si phase, preventing the formation and growth of an Al−Fe IMCs. Eventually, a micron ultrathin interface reaction layer composed of Al0.7Fe3Si0.3, FeAl, and Fe3Al phases is formed at the aluminum/steel welding interface. The maximum average shear strength of the joint is 176 MPa. The shear fracture is a typical ductile fracture. Properly reducing the friction speed and increasing the upsetting pressure can improve the bonding strength of aluminum/steel joints.

5 February 2026 in Metals
Verified
Journal Article
Open access
PDF file
YFYangfan Fu
Yangfan Fu
DCDa Long Cong
Da Long Cong
THTao Hu
Tao Hu
Guangjie FengGuangjie Feng
Guangjie Feng
ZLZhong Sheng Li
Zhong Sheng Li
Dean DengDean Deng
Dean Deng
This study systematically investigates the microstructure evolution, mechanical properties, and residual stress distribution in diffusion-bonded joints between Al2O3 ceramic and TC4 alloy. Motivated by the need for reliable high-temperature joints in advanced applications, this work addresses the challenges posed by the materials’ physicochemical differences. Joints were fabricated at temperatures ranging from 800 °C to 950 °C under a pressure of 3 MPa for 2 h. Microstructural characterization revealed the formation of a multi-layered interfacial structure, dominated by a Ti3Al reaction layer, whose thickness increased with bonding temperature. The highest shear strength of 54 MPa was achieved at 850 °C, representing a key quantitative outcome of this parameter optimization. Beyond this temperature, excessive growth of the brittle Ti3Al layer and associated residual stresses led to strength degradation and interfacial cracking. A three-dimensional finite element model was developed to simulate residual stress distributions, highlighting significant tensile stresses within the Ti3Al layer and compressive stresses in the Al2O3 near the interface. The model further identified critical tensile stress concentrations along the vertical edges of the ceramic, which contribute to failure during shear testing.

30 August 2026 in Applied Sciences
Verified
Journal Article
Open access
PDF file
YBYixin Bai
Yixin Bai
KSKaiqiang Song
Kaiqiang Song
XWXuan Wang
Xuan Wang
LYLei Yu
Lei Yu
AHAnwei Huang
Anwei Huang
ZLZhong Sheng Li
Zhong Sheng Li
Lightweight fiber-reinforced phenolic-resin aerogel (NF/PRA) composites are key ablation thermal protection materials for hypersonic vehicles. However, how resin precursor solid content governs the complete processing–structure–property chain, particularly the multi-mode mechanical behavior and high-heat-flux ablation performance, remains poorly understood. In this study, high-silica fiber/phenolic-resin aerogel composites with different contents of a novolac resin precursor (15%, H15S15; 20%, H15S20; 25%, H15S25; 30%, H15S30) were fabricated via vacuum-assisted resin transfer molding combined with atmospheric-pressure drying, and were systematically characterized in terms of their microstructure, mechanical properties, thermophysical behavior, thermal insulation, and ablation resistance. A higher solid content created a denser three-dimensional nano-network in the PRA matrix, decreasing the average pore size from 75.4 to 37.4 nm and increasing the bulk density from 0.299 to 0.458 g/cm3. The abundant mesopores led to ultra-low thermal conductivities of 0.039–0.042 W/(m·K). The compressive, flexural, and shear strengths increased monotonically with the solid content, whereas the tensile strength peaked at 18.03 MPa for H15S25 and declined at higher contents owing to matrix brittleness. Notably, a higher solid content synergistically enhanced both thermal insulation and ablation resistance. After oxyacetylene flame ablation, the linear ablation rate of H15S30 was 32.7% lower than that of H15S15, and the back-face temperature was more than 58% lower. Post-ablation microstructural observations revealed a three-stage mechanism involving pyrolytic carbonization, fiber melting, and mechanical scouring, in which layer-by-layer spallation of the amorphous carbon and SiO2-rich molten phases governs the damage. This study provides guidance for optimizing the processing–structure–property relationship of NF/PRA composites for ablation thermal protection applications.