The aim of the present study was to evaluate and quantify the damping properties of common resin-based computer-aided design and computer-aided manufacturing (CAD/CAM) restorative materials (CRMs) and assess their energy dissipation abilities. Leeb hardness (HLD), together with its deduced energy dissipation data (HLDdis), and loss tangent values recorded via dynamic mechanical analysis (DMA) were determined for six polymer, four composite, and one ceramic CRM as well as one metal. Data were statistically analyzed. Among resin-based CRMs, the significantly highest HLDdis data were detected for the fiber-reinforced composite FD (p < 0.001) directly followed by the filler-reinforced Ambarino High Class (p < 0.001). The significantly lowest HLDdis values were observed for the polymer-based CRM Telio CAD (p < 0.001). For loss tangent, both PEEK materials showed the significantly lowest data and the polymer-based M-PM the highest results with all composite CRMs in between. HLDdis data, which simultaneously record the energy dissipation mechanism of plastic material deformation, more precisely characterize the damping behavior of resin-based CRMs compared to loss tangent results that merely describe viscoelastic material behavior. Depending on material composition, resin-based CRMs reveal extremely different ratios of viscoelastic damping but frequently show enhanced HLDdis values because of plastic material deformation. Future developments in CAD/CAM restorative technology should focus on developing improved viscoelastic damping effects.
1 February 2022 in Journal of the Mechanical Behavior of Biomedical Materials
Objectives: This study evaluated the impact of mutable water uptake on the durability of mechanical properties and the long-term reliability of artificial composites. Methods: Three resin-based CAD/CAM restorative materials (CRMs) were investigated in three-point bending tests to calculate flexural strength (FS), modulus of elasticity (ME), modulus of resilience (MR), modulus of toughness (MT), and elastic recovery (ER). All specimens (n = 180) were stored under the same conditions and tested in four subsets (n = 15 per material) that were respectively withdrawn after repeated thermocycling (5000 cycles; 5–55 °C, H2O) and repetitive drying (7 d; 37 °C, air). For every specimen, weight differences were determined per storage condition. Likewise, loss tangent data were separately recorded via dynamic mechanical analysis to reliably assess damping characteristics. Results: Repeated thermocycling always induced weight increase and a concurrent significant loss in all mechanical properties except for MT and ER of a polymethylmethacrylate-based CRM. Drying consistently provoked weight loss and raised mechanical properties to initial values. Weight increase, however, enhanced loss tangent values and accordingly distinct damping characteristics, whereas weight decrease markedly lowered damping properties. Significance: Water uptake repeatedly induced a decrease in common mechanical properties but concurrently increased damping behavior. Invertible equilibrium processes were found with no evidence for permanent material degradation.