Representative Publications

View All Publications
26 November 2021 in Metals
Verified
Journal Article
Open access
PDF file
NNNatan Nudelis
Natan Nudelis
Peter MayrPeter Mayr
Peter Mayr
Nowadays, additive manufacturing (AM) using laser powder bed fusion (LPBF) is acknowledged for its ability to generate near-net-shape components for various industries such as aerospace, automotive, and health industries. However, internal defects seem to be the inevitable concomitant in the current state of laser powder bed fusion of Al alloys. Hence, knowledge of the formation, different types, and morphologies of pores and their suppression is an essential element for successful future AM applications. The purpose of this research is to qualify a new approach of defect classification using X-ray tomography. In this framework, this research examined the influence of size, shape, and location of pores on crack initiation for AlSi10Mg parts produced by LPBF. For this reason, a total number of 39,228 pores detected in a cylindrical sample were categorised. Additionally, 26 selected pores of different morphology from the X-ray scan were analysed by means of finite element analysis (FEA). Moreover, fracture mechanics determinations were carried out to examine the correlations between pore characteristics and degree of stress concentration. The result is an evaluated novel pore classification method that can be used for process adjustments, quality assurance, as well as further research.

10 November 2022 in The International Journal of Advanced Manufacturing Technology
Verified
Journal Article
Open access
PDF file
NNNatan Nudelis
Natan Nudelis
Peter MayrPeter Mayr
Peter Mayr
Due to high production costs and a limited reproducibility of quality, the high potential of laser powder bed fusion (LPBF) has not been fully exploited yet. In fact, internal defects can have a detrimental effect on the fatigue behaviour and cause final component failure. Therefore, process-induced defects must be localized and evaluated at a higher level of detail. The present study deals with the correlation amongst pores and LPBF process parameters in AlSi10Mg components. Computed tomography (CT) allows an extensive examination of internal defects. Within this work, a total number of 2,939,830 pores detected in 96 cylindrical samples were analysed using CT. The formation of pores can be adjusted by varying the modified volume energy density, for example, by using various laser scanning speeds. Furthermore, the effect of powder preparation scan strategies (pre-heating and pre-sintering) on the formation of different pore types as well as the general reproducibility was examined. For instance, the shielding gas flow, contaminated protective windows of the lasers as well as prior powder preparation influence the formation of pores. Using prior laser powder preparation reduced the total number of pores at high scanning speeds up to 45%. When the scanning speed is increased, the number of spherical pores decreases and large and irregularly shaped pores appear. Interestingly, only the pre-heating process resulted in a reduced formation of spherical pores at low scanning speeds (1000 mm/s).

14 September 2023 in Journal of Materials Science
Verified
Journal Article
Open access
PDF file
NNNatan Nudelis
Natan Nudelis
Peter MayrPeter Mayr
Peter Mayr
Despite past scientific efforts and the increased use of hot isostatic pressing (HIP) in additive manufacturing applications, a complete understanding of the exact pore-closing behaviour has yet to be achieved. The present research focuses on laser powder bed fused (LPBF), hot isostatic pressed components made of AlSi10Mg, and process-related defects. The study shows the effect of HIPing in relation to various pore characteristics, such as pore shape, size, and type. A pore tracing method using X-ray data was developed to characterise the pores before and after HIP. The method is based on the k-nearest neighbours approach and allows to match leftover pores with the initial ones. Hence, the efficiency of the pore-closing behaviour for different HIP settings can be analysed. Moreover, the exact number of pore transformations can be tracked, providing a comprehensive insight into the change of pore characteristics during HIP. In this framework, eight different HIP settings and a total number of 274,886 pores were examined and discussed. The findings demonstrate that longer treatment times and higher pressure and temperature settings accelerated the pore transformation. Irregularly shaped and large pores close faster than spherically shaped and smaller ones. Furthermore, regardless of the initial pore type, all pores started transforming their shape towards irregular shapes and small pore diameters. Some pores remained after the HIP treatments, probably due to the inefficiency of HIP in closing pores connected with the component surface or the presence of oxide particles interfering with the diffusion bonding process.