Magnetron sputter deposition was applied to grow thin metal films in the presence of impurities. These impurities are ambient gas molecules and/or atoms from the residual gas present in the vacuum chamber. Seven materials were investigated: four single element metals (Al, Ag, Cu, and Cr), two widely applied alloys (Cu55Ni45 and Ni90Cr10), and one high entropy alloy (CoCrCuFeNi). The thin films were analyzed using X-ray diffraction to determine the domain size, the film texture, and the lattice parameter. The same trend for all studied materials is observed. When the ratio between the impurity and metal flux towards the substrate is low, the domain size is not affected by the presence of the impurities. In this regime, the incorporation of the impurities affects the lattice parameter. At high flux ratios, the change of the domain size can be described by a power law with the exponent equal to −1/2 for all studied materials. A kinetic Monte Carlo code is used to demonstrate this observed trend.
CuO and Al thin films were successively deposited using direct current (reactive) magnetron sputter deposition. A multilayer of five bilayers was deposited on glass, which can be ignited by heating a Ti resistive thin film. The velocity of the reaction front which propagates along the multilayer was optically determined using a high-speed camera. During the deposition of the aluminum layers, air was intentionally leaked into the vacuum chamber to introduce impurities in the film. Depositions at different impurity/metal flux ratios were performed. The front velocity reaches a value of approximately 20 m/s at low flux ratios but drops to approximately 7 m/s at flux ratios between 0.6 and 1. The drop is rather abrupt as the front velocity stays constant above flux ratios larger than 1. This behavior is explained based on the hindrance of the oxygen transport from the oxidizer (CuO) to the fuel (Al).