Accurate estimation of cable tension is crucial for the structural health monitoring of cable-supported structures. Identifying the cable’s force from its vibration data is probably the most widely adopted method of cable tension estimation. According to string theory, the accuracy of estimated cable tension is highly related to identified modal parameters including natural frequencies and frequency order. To alleviate the factors that impact the accuracy of modal parameters when using the peak-picking method in wireless sensor networks, a fully automated and robust identifying method is proposed in this paper. This novel method was implemented on the Xnode wireless sensor system and validated with the data obtained from Jindo Bridge. The experiment results indicate that, through this method, the wireless sensor is able to distinguish the cognizable power spectrum, extract the peaks, eliminate false frequencies and determine frequency orders automatically to estimate cable tension force without any manual intervention or preprocessing. Meanwhile, the results of natural frequencies, corresponding orders and cable tension force obtained from the Xnode system show excellent agreement with the results obtained using the Matlab program method. This demonstrates the effectiveness and reliability of the Xnode estimation system. Furthermore, this method is also appropriate for other high-performance wireless sensor network systems to realize self-identification of cable in long-term monitoring.
Shear strength, which indicates the interfacial bond performance between new and old concrete, is critical in the field of structural reinforcement and rehabilitation. However, the absence of standardized testing equipment has hindered the accurate quantification of this parameter. To address this gap, a dedicated shear-loading apparatus was designed in this study, and finite element modeling was conducted to simulate the shear performance of concrete with different interface roughness. The results show that failure consistently occurs at the interface and that roughness has significant influence on shear capacity. In order to reveal the relationship between shear strength and surface roughness, shear experiments were conducted on new–old concrete using the device we designed. The surface of old concrete was treated by water-jetting, electric hammering, grooving, or grout seal strip to create different profiles, the roughness was quantified by 3D scanning and Fourier transform analysis, and fresh concrete was then cast atop the processed surfaces to form composite specimens. The results show that the correlation between shear strength (τ) and Fourier transform roughness (FTR) can be described with the equation τ (MPa) = 0.546FTR2 + 1.832FTR − 0.447.
To promote construction waste recycling and develop sustainable pavement materials, this study utilized recycled aggregates (crushing value 7.8%) obtained from bridge demolition as a 100% replacement for natural aggregates in recycled pervious concrete. The research focused on investigating the influence of different aggregate gradations (single-sized 4.75–9.5 mm and binary-graded combinations: 4.75–9.5 + 16–31.5 mm, 2–5 + 13–26.5 mm) and different water-to-cement ratios (0.26, 0.27, 0.30) on the concrete properties. Tests on compressive strength, splitting tensile strength, and connected porosity revealed the following results: The strength of recycled pervious concrete was comparable to that of natural aggregate concrete, and strength decreased with increasing aggregate size. The optimal water-to-cement ratio varied with gradation: 0.27 for the single-sized 4.75–9.5 mm aggregate and 0.30 for the binary-graded combinations. Splitting tensile strength was generally low, showed insignificant growth from 7 d to 28 d, was sensitive to interfacial defects, and exhibited high data variability. Connected porosity was inversely proportional to compressive strength and decreased with increasing water-to-cement ratio. This study provides experimental evidence for optimizing the preparation of high-performance recycled pervious concrete using recycled aggregates. In addition, the influence of fiber type, dosage, and length was preliminarily examined through an orthogonal design.
The regulatory mechanism of vinyl acetate-ethylene (VAE) in the interfacial properties of silicate cement–silica fume repair mortar was investigated by examining the effects of varying VAE contents (0 wt.% to 10.0 wt.%) on mortar fluidity, mechanical strength, and interfacial bonding strength. The interface microstructure was also examined to reveal its evolution. Results indicate that VAE enhances mortar fluidity through micro-filling and interfacial activity. At 10% VAE content, fluidity reached 265 mm, a 14.97% increase. However, VAE introduction reduced compressive and flexural strength due to pore induction at low dosages and polymer network interference at high dosages. By improving interfacial stress transfer and refining calcium sulfoaluminate (AFt) and C-S-H crystals in the interfacial transition zone, VAE increased the tensile bonding strength of the repaired mortar to 2.1 MPa at 28 days, a 133.3% increase, according to microscopic analysis. Based on performance analysis, 5.0 wt.% VAE is optimal, increasing interfacial bonding strength by 133.3% while limiting compressive strength loss to 9.4%, thus achieving interfacial collaborative optimization of the repaired mortar.
About Me
College of Water Conservancy and Civil Engineering, South China Agricultural University,Guangzhou 510642, PR China.
College of Water Conservancy and Civil Engineering, South China Agricultural University,Guangzhou 510642, PR China.