A series of novel hierarchical nanoporous microstructures have been synthesized through one-step chemical reduction of micron size Cu2O and Co3O4 particles. By controlling the reduction time, non-porous Cu2O microcubes sequentially transform to nanoporous Cu/Cu2O/Cu dented cubic composites and hollow eightling-like Cu microparticles. The mechanism involved in the complex structural evolution is explained based on oxygen diffusion and Kirkendall effect. The nanoporous Cu/Cu2O/Cu dented cubic composites exhibit superior electrochemical performance as compared to solid Cu2O microcubes. The reduction of nonporous Co3O4 also exhibits a uniform sequential reduction process from nonporous Co3O4 to porous Co3O4/CoO composites, porous CoO, porous CoO/Co composites and porous foam-like Co particles. Nanoscale channels originate from the particle surface and eventually develop inside the entire product, resulting in porous foam-like Co microparticles. The Kirkendall effect is believed to facilitate the formation of porous structures in both processes.
High-performance microwave absorbing materials require optimized impedance matching and high attenuation ability. Here we meet the challenge by incorporating electric loss with magnetic loss materials to prepare carbon-based/magnetic hybrids. The reduced graphene oxide (rGO)/La0.7Sr0.3MnO3 (LSMO) composites were prepared by dispersing the LSMO powders into 4.25, 6.25, 8.16, and 10 wt% of the graphene oxide aqueous solution, then the rGO/LSMO composites were formed by hydrothermal method. The pure rGO, LSMO, and rGO/LSMO composites were studied using X-ray diffraction and SEM. Microwave absorption properties were investigated by using coin method. Simulation studies show that 6.25 wt% of rGO/LSMO in a wax matrix exhibits the strongest reflection loss of −47.9 dB @ 10.7 GHz at a thickness of 2.5 mm. Moreover, the effective absorption bandwidth with the reflection loss below −10 dB is up to 14.5 GHz, ranged from 3.5 to 18 GHz for the composites with a thickness of 1.5–5.5 mm, due to a synergism between dielectric loss of rGO and magnetic loss of magnetic LSMO, which is an interesting exploration in the applications of rGO and LSMO. This method can be extended to design and fabricate hybrid absorbers with effective microwave absorption.
In this work, we performed a systematic study of the physical properties of amorphous Indium–Gallium–Zinc Oxide (a-IGZO) films prepared under various deposition pressures, O/(Ar+O) flow ratios, and annealing temperatures. X-ray reflectivity (XRR) and microwave photoconductivity decay (-PCD) measurements were conducted to evaluate the quality of a-IGZO films. The results showed that the process conditions have a substantial impact on the film densities and defect states, which in turn affect the performance of the final thin-film transistors (TFT) device. By optimizing the IGZO film deposition conditions, high-performance TFT was able to be demonstrated, with a saturation mobility of 8.4 cm/Vs, a threshold voltage of 0.9 V, and a subthreshold swing of 0.16 V/dec.