Magnesium (Mg) alloys are a very attractive material of construction for biodegradable temporary implants. However, Mg alloys suffer unacceptably rapid corrosion rates in aqueous environments, including physiological fluid, that may cause premature mechanical failure of the implant. This necessitates a biodegradable surface barrier coating that should delay the corrosion of the implant until the fractured/damaged bone has healed. This review takes a brief account of the merits and demerits of various existing coating methodologies for the mitigation of Mg alloy corrosion. Since among the different coating approaches investigated, no single coating recipe seems to address the degradation control and functionality entirely, this review argues the need for polymer-based and biodegradable composite coatings.
The electrochemical stability of the buried metal-organic coating interface of painted metal is crucially governed by how effectively the oxygen reduction reaction at the interface is inhibited. As this interface is not directly accessible for study by conventional electrochemical techniques, a new non-destructive method has been developed wherein hydrogen permeation is used to quantitatively measure the oxygen reduction kinetics underneath the coatings. Presented here are results obtained with an adaptation of the Devanathan-Stachurski cell where the oxygen reduction reaction kinetics on the coated exit is probed by monitoring the dynamic electrochemical equilibrium potential established as a result of oxygen reduction and hydrogen oxidation reactions. From the hydrogen uptake on the entry side thus a full current-potential relationship curve (I (U)) can be constructed. First tested on non-coated Palladium, the results show very good concurrence of the oxygen reduction currents from the permeation experiments and that from standard cyclic-voltammetry (CV) measurements in buffered and non-buffered acidic electrolyte and under alkaline condition. Initial results obtained on coated samples are also presented
28 September 2016 in Journal of the Electrochemical Society
Corrosion driven delamination of coatings is crucially determined by the rate of the cathodic oxygen reduction reaction at the buried metal-organic coating interface. Quantitative measurement of this rate at such interfaces by conventional techniques is impeded due to the blocking of ion transport by the coating. A new approach where hydrogen permeation is used as a tool to measure the oxygen reduction rate underneath coatings has been recently introduced. This permeation based potentiometry approach measures the rate of the oxygen reduction reaction by correlating the open circuit potential established as a consequence of the dynamic electrochemical equilibrium between hydrogen oxidation and oxygen reduction reactions on the coated exit side with the hydrogen uptake rate on the entry side. In this work, the interfacial reaction kinetics of the oxygen reduction reaction causing delamination of the coating are investigated by this hydrogen permeation based potentiometric approach. Moreover, thus performed prolonged cathodic polarizations of the palladium/coating interface have been found to destroy the interface, just like it is the case in the cathodic delamination process. Initial results obtained on ultra-thin films of iron on palladium are also presented, showing that the technique is applicable also on technically more relevant metal surfaces.
30 December 2024 in International Journal of Hydrogen Energy