Scanning tunnel microscopy is used to directly estimate the relative energy of internal interfaces in ultrafine-grained copper after equal-channel angular pressing, followed by rolling. Estimates of the boundary energy for as-prepared samples and samples annealed at different temperatures indicate that ultrafinegrained copper has nonequilibrium boundaries with energy higher than that in coarse-grained copper. The cumulative distribution functions of the relative boundary energy in the grain–subgrain structure allow the qualitative estimation of the redistribution of excess energy between the boundaries of various types during structure evolution upon annealing. Differences between the behaviors of the cumulative distribution functions of relative boundary energy in ultrafine-grained copper and nickel produced by the same technology are revealed. These differences are related to the characteristics of the structure formation of two metals during severe plastic deformation and its subsequent evolution during annealing, which depend on the stacking fault energy and the melting point of copper and nickel.
Using the method of measuring the positron lifetime spectra and Doppler broadening annihilation line spectroscopy, the annealing of defects in submicrocrystalline nickel produced by equal channel angular pressing has been studied. In as-prepared samples, the positrons are trapped by dislocation defects and vacancy complexes inside crystallites. The size of vacancy complexes decreases with increasing annealing temperature in the interval ΔT = 20–300°C. However, at T = 360°C, the complexes start growing again. The dependence of S-parameter on W-parameter derived from the Doppler broadening spectroscopy has two parts with different inclinations to axes that correspond to different types of primary centers of positron trapping in submicrocrystalline nickel. It has been elucidated that, at recovery stage in the temperature interval ΔT = 20–180°C, the main centers of positron trapping are low-angle boundaries enriched by impurities, while at in situ recrystallization stage in the temperature interval ΔT = 180–360°C, the primary centers of positron trapping are low-angle boundaries.
This paper presents the results of a defect structure investigation in commercially pure titanium alloy after hydrogen charging in a gaseous atmosphere at the temperature of 873 K up to the concentration of 5.1 at. %. Structure of samples was studied by positron lifetime, Doppler broadening and X-ray diffraction spectrometry. Several processes, corresponding to the different ranges of hydrogen concentrations were revealed. It was shown that hydrogen, penetrating in the material, expands its crystal lattice, initiates formation of vacancy-like defects of different dimensions and reacts with the last ones, forming the defect-hydrogen complexes.
The influence of ultrasonic plastic treatment (UPT) on the relief, microstructure, and phase state of the surface of nickel titanium (TiNi) has been studied. The UPT leads to significant hardening, nanofragmentation, and a change in the phase state of the surface TiNi layer.