The weak interface performance between metal and composite (IPMC) makes the composite materials susceptible to impact load. Aluminum/glass fiber/polypropylene (Al/Gf/PP) laminates were manufactured with the aluminum alloy sheets modified by nitrogen plasma surface treatment and the phosphoric acid anodizing method, respectively. FEM models of Al/Gf/PP laminates under low-velocity impact were established in ABAQUS/Explicit based on the generated data including the model I and II interlaminar fracture toughness. Low-velocity impact tests were performed to investigate the impact resistance of Al/Gf/PP laminates including load traces, failure mechanism, and energy absorption. The results showed that delamination was the main failure mode of two kinds of laminates under the impact energy of 20 J and 30 J. When the impact energy was between 40 J and 50 J, there were metal cracks on the rear surface of the plasma pretreated specimens, which possessed higher energy absorption and impact resistance, although the integrity of the laminates could not be preserved. Since the residual compressive stress was generated during the cooling process, the laminates were more susceptible to stretching rather than delamination. For impact energy (60 J) causing the through-the-thickness crack of two kinds of laminates, plasma pretreated specimens exhibited higher SEA values close to 9 Jm2/kg due to better IPMC. Combined with the FEM simulation results, the interface played a role in stress transmission and specimens with better IPMC enabled the laminates to absorb more energy.
The effects of pre-deformation and artificial aging on fatigue life of 2198 Al-Li alloy were explored to further reveal its fatigue behavior and improve the damage tolerance. Fatigue life was investigated on 2198-T3 alloy after pre-deformation and aging treatments. Scanning electron microscopy (SEM) and transmission electron microscopy (TEM) were used to study the fracture morphology, precipitation behavior, fatigue crack initiation and propagation. Results indicated that T1 (Al2CuLi) phase dominated the strengthening of 2198-T3 alloy after the further aging. Pre-deformation increased the number of dislocations in the matrix, which provided favorable position for nucleation of T1. The precipitation of θ′ (Al2Cu) and δ′ (Al3Li) were inhibited. Also, the formation and coarsening of precipitate-free zone (PFZ) were effectively avoided in this condition. Dislocation density in the 2198 Al-Li alloy matrix increased with the amount of pre-deformation, leading to an increase in micro-crack defects on the surface and inside alloy. As a result, decreased fatigue life and an increased crack growth rate of the alloy were observed. Overall, 2198 Al-Li alloy had the best fatigue life and damage tolerance enhancement after it underwent 3% pre-deformation and was aged at 155 °C for 15 h.
24 January 2018 in The International Journal of Advanced Manufacturing Technology
Flow behaviors of 22MnB5 ultra-high strength steel (UHSS) at different temperatures and strain rates were investigated using uniaxial tension tests. The variables of the Arrhenius model, which involved n, Q, α, and lnA, was calculated using a fifth order polynomial fitting method. At a strain of 0.1, the values of n, Q, α, and lnA were respectively 8.24579, 177.7588 kJmol-1, 0.00618 MPa-1, and 25.77352 s-1. The results indicate that the change in rheological stress was inversely proportional to the change in temperature but was positively correlated with the change in strain rate. The new model reproduced the flow behaviors of this novel UHSS sheet well for a wide range of strain rates and temperature conditions.