The purpose of this study is the surface modification of a micro-sized nanoporous zeolite through a silylation reaction and the incorporation of the silylated particles into a homogeneous cellulose acetate (CA) membrane to achieve better polymer-zeolite adhesion in the corresponding mixed matrix membranes (MMMs). In the current study, 3-aminopropyl(diethoxy)methylsilane (APDEMS) was used as the silane coupling agent and micro-sized nanoporous sodium zeolite-Y (NaY) as the precursor zeolite. The unmodified pure form of the zeolite (NaY), the silane-modified zeolite (NaY-sm) and the corresponding MMMs were characterized using DLS, BET, FTIR-ATR, XRD, SEM, and TG/DTA analyses. Moreover, the CO2/N2 separation performances of the prepared membranes were evaluated through the gas permeation measurements. The results demonstrated that the modification results in an increase in average particle diameter, external surface area, and overall volume (or size) as well as a decrease in the micropore surface areas, volumes, and the crystallinities of the resultant modified zeolite particles. In addition, the modification led to an improvement in the uniformity of the particle distributions all over the MMM structure and a considerable reduction in the numbers/sizes of the undesirable cracks and agglomerates. The CO2 permeability of CA increased about 77.19% at 4 bar for the CA/NaY-sm 20 wt% membrane. It could be almost concluded that not only did the CO2 permeability of CA/NaY-sm membranes not decrease when compared to CA/NaY membranes, but the permeability also actually showed an average 4.67% increase. Moreover, an average CO2/N2 selectivity of 6.34% was obtained for NaY-sm filled MMMs compared to those filled with the pure NaY (≥4 bar). This can be a significant contribution to developing new materials in the field.
In this work, a newly engineered alumina quantum dot-based nanofluid (α-AQDs; D ~ 4 nm; amorphous solid) and one commercial alumina nanoparticle-based nanofluid (γ-ANPs; D ~ 20 nm; crystalline type) with the capability of strong colloidal dispersion at reservoir conditions, such as, high salinity, divalent ions (Ca2+) and high temperature was compared. The main goal of this research was to study the crude oil displacement mechanisms of alumina suspensions as a function of variety in size and particle morphology in aged carbonate rocks. The strong interaction potential between the particles was achieved by the citric acid and a special composition of a carboxylate-sulfonate-based polyelectrolyte polymer as an effective dispersant compound on the surface, leading to a negative particle charges and an additional steric and electrostatic repulsion. Wettability alteration upon exposure to fluids using the contact angle and the Amott cell were performed on saturated carbonate plug samples and rock slices. While, dynamic core displacements were conducted to test the water/nanofluid/oil flow and nanoparticle retention behavior thorough typical pore throats underground the reservoir conditions. The stability results revealed that PE-polymer was able to create a long-term colloidal fluid during 30 days. It was found that mass concentration of nanofluid increased with decreasing in particle size. The optimal amount of particles in aqueous solution was obtained 0.05 wt% for ANPs, increased up to 0.1 wt% for AQDs. Analysis of experiments showed that wettability alteration was the main mechanism during nanofluid injection. Laboratory core-flooding data proved that the enhanced oil recovery due to a less concentration state by ANPs was consistent with AQDs at higher concentrations. In addition, permeability-impairment-behavior study was discussed in terms of possible mineral scale deposition and alumina release on the rock surface. Results showed that a large extent of permeability damage caused by mineral scale (55–59%). Alumina quantum dot-based nanofluids were found a minimum impairment (2–4%) and a significant reduction of ~ 10% in permeability was observed for ANPs-based nanofluid.