Zinc sulfide (ZnS) thin films have been deposited on Si (1 0 0) substrate using ultrasonic spray pyrolysis. X-ray diffraction (XRD) analysis revealed that the films are (0 0 2) preferentially oriented with c-axis-oriented wurtzite structure. The crystallinity has been found to improve with film thickness in the 180–6000 nm range. Film structure has been analyzed by XRD, scanning electron microscope, FTIR, and Raman spectroscopies, while the stoichiometry has been verified by energy-dispersive spectroscopy and particle-induced X-ray emission techniques. Electrical properties of the grown films were characterized by current–voltage and capacitance–voltage measurements where, the films show better conducting behavior at higher thickness.
Na2WO4 films have been grown on Si (1 0 0) and glass substrate using ultrasonic spray pyrolysis. The films are prepared from aqueous solution containing Na2WO4·2H2O at 475 °C temperature and characterized by XRD and SEM techniques and the chemical composition of the films have been verified by EDX and PIXE and its formula Na2WO4 is confirmed by XRD. The evolution of the crystallinity was studied as a function of film thickness ranging from 2500 to 4200 nm, which corresponds to a deposition time from 10 to 30 min, respectively. The crystalline quality was found to improve, where the grain size values increased with increasing thickness. Atomic Force Microscopy (AFM) was used to study the morphology evolution with the deposition time, where porous films were found due to the synthesis parameters, and a better sensing response to gases was developed with increasing thickness. Thus, this study demonstrates the possibility of utilizing Na2WO4 thick films as a sensor element for the detection of ethanol vapor at room temperature, where thicker films exhibit excellent ethanol vapor sensing properties with a maximum sensitivity at 25 °C in air atmosphere with fast response time.