There is growing interest in sustainable road pavement technologies to protect the environment and provide economic benefits. Post-consumer recycled (PCR) plastics are considered for construction to address the threat of plastic waste materials (PWM) and to improve sustainability. Asphalt pavement construction is highly considered for PWM recycling due to its large daily production. The purpose of this study is to investigate the performance of asphalt mixture containing PWM, specifically high-density polyethylene (HDPE), and compare its performance with two conventional mixtures. Three asphalt mixtures were considered: (1) mixture with asphalt binder PG 76-22 (SBS-modified); (2) mixture with asphalt binder PG 70-22 (SBS-modified); and (3) mixture with binder PG 67-22 and 3% HDPE (the plastic mixture). The rheological properties of the modified asphalt binders and the performance of the modified asphalt mixtures were evaluated. The long-term field performance of the pavements was modeled using AASHTOWare software (v.1.1.6) for the three mixtures considered. The results showed that all the mixtures were able to comply with the cracking threshold specified by the Louisiana Department of Transportation and Development (LaDOTD) for high-traffic volume roads. In addition, the plastic asphalt mixture showed similar performance to the one containing PG 70-22 (SBS-modified) asphalt binder.
The aim of the research is to quantify the property of asphalt mortar and asphalt mixture containing municipal solid waste incineration (MSWI) fly ash. The potential of partially replacing mineral fillers with MSWI fly ash in asphalt mixture production was investigated. Five different MSWI fly ash replacement ratios, which include 0%, 25%, 50%, 75%, and 100%, were adopted to assess the influence of fly ash dosage, and the optimum fly ash replacement ratio was proposed. The rheological characteristics of asphalt mortar with MSWI fly ash were assessed with the dynamic shear rheometer (DSR) and bending beam rheometer (BBR). The high temperature properties of the mixture with MSWI fly ash were assessed with the Marshall stability test and the rutting test. The low temperature cracking property was determined with the indirect tensile strength test at low temperatures. The moisture stability property was identified with the immersed Marshall test and the freeze-thaw cycles conditioned indirect tensile strength test. Based on the test results, the addition of fly ash and mineral filler remarkably increased the ǀG*ǀ of the asphalt mortar. The δ of asphalt decreased as the dosage of fly ash and mineral filler increased. The addition of fly ash and mineral filler degraded the low temperature characteristics of the mortar. Fly ash improved the high temperature characteristics of the asphalt mixture. The asphalt mixture with MSWI fly ash was more susceptible to thermal cracking than the control sample. The addition of fly ash weakened the moisture stability of the asphalt mixture. In order to guarantee the low temperature characteristics and the moisture susceptibility of the asphalt mixture, the fly ash replacement ratio was recommended to be set around 25%. With proper mixture design and fly ash dosage, the asphalt mixture would have adequate performance, as well as reduced environmental impact.