1 July 2020 in Construction and Building Materials
Verified
Journal Article
Closed access
HLHua Li
Hua Li
YWYi Wang
Yi Wang
YWYujiang Wang
Yujiang Wang
JLJiaping Liu
Jiaping Liu
QTQian Tian
Qian Tian

1 May 2018 in Construction and Building Materials
Verified
Journal Article
Closed access
HLHua Li
Hua Li
QTQian Tian
Qian Tian
HZHaitao Zhao
Haitao Zhao
ALAnqun Lu
Anqun Lu
JLJiaping Liu
Jiaping Liu

1 October 2020 in Construction and Building Materials
Verified
Journal Article
Closed access
HZHaitao Zhao
Haitao Zhao
YXYu Xiang
Yu Xiang
DXDongsheng Xie
Dongsheng Xie
WXWen Xu
Wen Xu
YWYujiang Wang
Yujiang Wang
JLJiaping Liu
Jiaping Liu

1 October 2020 in Magazine of Concrete Research
Verified
Journal Article
Closed access
HLHua Li
Hua Li
JLJiaping Liu
Jiaping Liu
YWYujiang Wang
Yujiang Wang
QTQian Tian
Qian Tian
The restrained volume expansion of expansive agents during hydration is often used to offset strains caused by the shrinkage of cement-based materials (CBMs). The hydration and expansion process of a laboratory-prepared calcium-oxide (CaO)-type expansive agent (CEA) in CBMs and modelling of the same are discussed in this paper. Based on isothermal calorimetry and thermogravimetry/differential thermal analysis, the hydration behaviour of the CEA in cement paste was examined, based on which the hydration kinetics were analysed and the apparent hydration activation energy of the CEA was calculated. Based on the degree of hydration, a chemo-mechanical model of the expansion of the CEA in CBMs was developed and analysed by comparison with experimental data obtained by the dual-ring restraint test method. Based on this model, it is possible to predict the expansion performance and crack resistance of concrete containing CEA agent.

28 January 2022 in Crystals
Verified
Journal Article
Open access
PDF file
YWYujiang Wang
Yujiang Wang
QTQian Tian
Qian Tian
HLHua Li
Hua Li
WWWang Wang
Wang Wang
Ultra-high performance concrete (UHPC) has a potential cracking risk due to its large autogenous shrinkage. The use of an expansive agent is an effective approach to reduce autogenous shrinkage of UHPC. However, different kinds of expansive agents show different expansive efficiency in UHPC. To study the cause for the difference in expansive efficiency, this study selected three expansive agents, namely highly reactive MgO-based, medium reactive MgO-based, and CaO-based expansive agents, and carried out the following experiments: autogenous shrinkage, hydration heat, hydration process of expansive agent under different relative humidity (RH), and micrographs. The results showed that the CaO-based expansive agent has high hydration activity at RH of more than 44.0%, while the hydration activity of two kinds of MgO-based expansive agents, especially a medium reactive MgO-based expansive agent, decreases significantly when RH drops below 80%. Meanwhile, the CaO-based expansive agent had higher expansive efficiency in UHPC than the MgO-based expansive agent. This study suggested that the CaO-based expansive agent is more suitable for compensating autogenous shrinkage of UHPC due to its low humidity sensitivity compared to the MgO-based expansive agent.

4 January 2023 in Materials
Verified
Journal Article
Open access
PDF file
JLJinyuan Lu
Jinyuan Lu
PFPan Feng
Pan Feng
HLHua Li
Hua Li
QTQian Tian
Qian Tian
In China, MgO-based expansive agent (MEA) has been used for concrete shrinkage compensation and cracking control for over 40 years. The expansive behavior of MEA in cementitious materials could be manipulated to some extent by adjusting the calcination process of MEA and influenced by the restraint condition of the matrix. It is key to investigate the factors related to deformation and cracking resistance so that the desired performance of MEA in certain concrete structures could be achieved. This paper reviews the influence of key parameters such as hydration reactivity, dosage, and calcination conditions of MEA, the water-to-binder ratio, supplementary cementitious material, aggregates, and curing conditions on the deformation and cracking resistivity of cement paste, mortar, and concrete with an MEA addition. The numerical simulation methods and deformation prediction models are then summarized and analyzed for more reasonable estimations.