In this work, black nanocarbon-loaded 0–100 parts-per-hundred (phr) PbO-filled acrylonitrile butadiene rubber (NBR)/styrene-butadiene rubber (SBR) blend composites were prepared by using an ordinary standard rubber mixer. Both mechanical and gamma attenuation properties of the prepared samples were investigated. Maximum tensile strength and elongation at break were obtained at 40 phr PbO concentration. The obtained values for the mass attenuation coefficient with the increased PbO concentration from 0–100 phr ranged from 0.12–0.22 cm2/g at 0.239 MeV. Scanning electron microscope (SEM) with the elemental mapping analysis results showed high homogeneity at 40 phr of the prepared rubber composites, with some areas of elemental agglomeration at a high concentration of lead oxide. The obtained results highly recommend the use of the prepared nanocarbon-reinforced PbO/NBR/SBR blend compared to those previously used as personal protective equipment in radiation-shielding applications.
The optimization of the TiO2 layer in free-hole perovskite solar cells is critical, as it strongly affects the device performance. In this study, simple FTO/TiO2/CH3NH3PbI3/C solar cells were fabricated, via two-step dipping method, with different thickness of TiO2 layer. The structure and microstructure of the TiO2 layers were investigated by X-Ray diffraction (XRD), Raman spectroscopy, and UV spectroscopy (UV-vis). The effect of different TiO2 thickness on the structure and photovoltaic performance of the fabricated devices were investigated using XRD and IV measurement, respectively. The photovoltaic parameters, including short-circuit-current (Jsc), open-circuit-voltage (Voc), Fill factor (F.F) and power conversion efficiency (PCE), were found to be strongly dependent on the thickness of TiO2 layer. The investigation showed that, efficient device can be fabricated by optimizing the TiO2 thickness, employing a thickness of 108 nm as an optimum thickness in this study.
23 November 2023 in Optical and Quantum Electronics