Elham Karami

Dr. Elham Karami

Department of Wood Processing and Biomaterials, Faculty of Forestry and Wood Sciences, Czech University of Life Sciences Prague
orcid

Research Focus & Metrics

Academic Career Length

17Years (2010-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
5 December 2010 in Notulae Scientia Biologicae
Verified
Journal Article
Open access
PDF file
EKElham Karami
Elham Karami
KPKambiz Pourtahmasi
Kambiz Pourtahmasi
MSMahdi Shahverdi
Mahdi Shahverdi
Wood Anatomical Structure of Morus alba L. and Morus nigra L., Native to Iran

21 January 2024 in Materials
Verified
Journal Article
Open access
PDF file
Tomáš KytkaTomáš Kytka
Tomáš Kytka
MGMiroslav Gašparík
Miroslav Gašparík
LSLukáš Sahula
Lukáš Sahula
DNDavid Novák
David Novák
EKElham Karami
Elham Karami
MSMartin Sviták
Martin Sviták
In this study, alder, spruce, and beech woods were used for homogeneous symmetric, inhomogeneous symmetric (combined) and inhomogeneous non-symmetric glued laminated timber (glulam) beams glued with resorcinol phenol formaldehyde (RPF) adhesive. The aim of this paper is to determine and compare the modulus of elasticity of glulam beams using three methods, i.e., analytical calculation, numerical model (FEM) and experimental testing. As an additional characteristic, the bending strength (MOR) of the beams was determined during experimental testing. Analytical calculation was used to calculate the modulus of elasticity (MOE) of glued laminated timber based on the knowledge of the modulus of elasticity of solid wood and to estimate the location of the neutral axis during bending. According to calculations, for symmetrical combinations, the deviation from the real neutral axis does not exceed 5%. In the case of the modulus of elasticity, the deviation is an average of 4.1% from that of the actual measured beams. The numerical model includes finite element modelling, where the deflection of the modelled beams can be calculated with a deviation of up to 10%. The last method was experimental testing of glued beams using four-point bending, in which, among homogeneous beams, beech glulam beams achieved the highest MOE and MOR, while alder glulam beams achieved the lowest. The combination of wood species resulted in an increase in both MOE and MOR compared to homogeneous spruce and alder beams.

2 December 2022 in European Journal of Wood and Wood Products
Verified
Journal Article
Closed access
PDF file
MGMiroslav Gašparík
Miroslav Gašparík
EKElham Karami
Elham Karami
TKTomáš Kytka
Tomáš Kytka
SDSumanta Das
Sumanta Das
THTomáš Houska
Tomáš Houska

22 February 2022 in Forests
Verified
Journal Article
Open access
PDF file
MGMiroslav Gašparík
Miroslav Gašparík
EKElham Karami
Elham Karami
FRFatemeh Rezaei
Fatemeh Rezaei
Tomáš KytkaTomáš Kytka
Tomáš Kytka
SDSumanta Das
Sumanta Das
DLDoubravka Lesáková
Doubravka Lesáková
This article deals with the effect of alternating lower (freezing) and higher (heating) temperatures on the static bending characteristics of glued Norway spruce (Picea abies (L.) H. Karst.) and European larch (Larix decidua Mill.) wood. Two types of wood, PUR (polyurethane), and EPI (emulsion polymer isocyanate), were used for the experiment. The thermal loading of glued wood was carried out at temperatures −15 °C/70 °C and −25 °C/70 °C. Static bending characteristics were determined on glued wood samples and compared with the reference samples. Freezing causes an increase in the bending properties of both glued spruce and larch wood. The highest in bending strength was obtained for EPI-glued larch wood subjected to −25 °C/70 °C loading temperature, which is by as much as 20% increase from the reference value. The maximum improvement in the modulus of elasticity was achieved for EPI-glued larch with around 11% increase, although the increased values of bending strength and modulus of elasticity were not significant. The different densities, anatomical structures, and properties of spruce and larch wood can induce varying results between the two wood species.

16 January 2024 in Fire
Verified
Journal Article
Open access
PDF file
Tomáš KytkaTomáš Kytka
Tomáš Kytka
MGMiroslav Gašparík
Miroslav Gašparík
DNDavid Novák
David Novák
LSLukáš Sahula
Lukáš Sahula
EKElham Karami
Elham Karami
SDSumanta Das
Sumanta Das
This study delved into the combustion properties of combined glulam bonded using polyurethane (PUR) and resorcinol-phenol-formaldehyde (RPF) adhesives. The experiment involved three distinct wood species, namely, spruce, alder, and beech, which were combined in homogeneous, non-homogeneous symmetrical, and non-homogeneous asymmetrical arrangements. These species were selected to represent a spectrum, namely, softwood (spruce), low-density hardwood (alder), and high-density hardwood (beech). The varying combinations of wood species illustrate potential compositions within structural elements, aiming to optimize mechanical bending resistance. Various parameters were measured during combustion, namely, the heat release rate (HRR), peak heat release rate (pHRR), mass loss rate (MLR), average rate of heat emission (ARHE), peak average rate of heat emission (MARHE), time to ignition (TTI), and effective heat of combustion (EHC). The findings indicate that incorporating beech wood into the composite glulam resulted in an increase in heat release, significantly altering the burning characteristics, which was particularly evident at the second peak. Conversely, the use of spruce wood exhibited the lowest heat release rate. Alder wood, when subjected to heat flux at the glued joint, displayed the highest heat emission, aligning with the results for EHC and MARHE. This observation suggests that wood species prone to early thermal decomposition emit more heat within a shorter duration. The time to ignition (TTI) was consistent, occurring between the first and second minute across all tested wood species and combinations. Notably, when subjected to heat flux, the glulam samples bonded with PUR adhesive experienced complete delamination of the initial two glued joints, whereas those bonded with RPF adhesive exhibited only partial delamination.

31 August 2022 in iForest - Biogeosciences and Forestry
Verified
Journal Article
Open access
PDF file
EKElham Karami
Elham Karami
IBI. Brémaud
I. Brémaud
SBS. Bardet
S. Bardet
TAT. Almeras
T. Almeras
DGD. Guibal
D. Guibal
JGJ. Gril
J. Gril
Thermal treatments can be considered as an accelerated ageing, bringing partly similar changes in properties as naturally aged wood. Thermal treatment was applied on white mulberry (Morus alba L.), a dominant species for making musical instruments from middle-East to Far-East, to investigate the effects on the vibro-mechanical and physical properties of this wood, and the results compared to previously published data on spruce (Picea abies Karst.) as a reference for the soundboard of Western string instruments. Thermal treatment (TT) at 150 °C and 0% of relative humidity was applied to five analogous groups of specimens with five different durations (2.5, 8, 24, 72, 261 hours). Humidity re-conditioning of specimens was done to explore the reversibility of TT effects. Physical and vibrational properties such as specific gravity (γ), equilibrium moisture content (EMC), CIELab colorimetric values, specific modulus of elasticity (E’/γ) and damping coefficient (tanδ) in longitudinal (L) and radial (R) directions, have been measured after stabilisation of samples in standard conditions (20 °C, 65% RH), before and after TT and then after re-conditioning. Untreated mulberry had a low EMC, very low L/R anisotropy and low E’L/γ, and relatively low tanδ. Weight loss (WL) and CIELab values evolved similarly during TT for mulberry and for previous results on spruce, however, their EMC and vibrational properties were affected differently. This could be explained in part by the low anisotropy of mulberry, and in part by its particular extractives. The parts of irreversible effects, linked to chemical modification or degradation, and of reversible effects, linked to physical configuration, were different between mulberry and spruce. The applied treatments did not bring permanent “improvements” in vibrational properties of mulberry, yet its colour appearance was enhanced.