The electromagnetic pulse (EMP) is a destructive phenomenon which harms the building, telecommunication, and IT based infrastructure. Thus, it is required to reduce the effect of EMP using shielding materials. In the present study, we have used different thickness of concrete walls by incorporating 1 and 5 wt% of carbon black, as well as 100 µm thick Zn–Al coating using the arc thermal metal spraying method (ATMSM). The EMP was evaluated using waveguide measurement fixture for shielding performance of the concrete wall in the range of 0.85 to 1 GHz frequency. The results reveal that the maximum value, i.e., 41.60 dB is shown by the 5-300-N specimen before application of Zn–Al coating where the thickness of concrete wall was 300 mm and 5% carbon black. However, once the 100 µm thick Zn–Al coating was applied on concrete specimen, this value was increased up to 89.75 dB. The increase in shielding values around 48 dB after using the Zn–Al coating is attributed to the reflection loss of the metal thermal spray coating. Thus, the Zn–Al coating can be used for EMP application instead of metallic plate.
Waste water treatment reservoirs are contaminated with many hazardous chemicals and acids. Reservoirs typically comprise concrete and reinforcement steel bars, and the main elements responsible for their deterioration are hazardous chemicals, acids, and ozone. Currently, a variety of techniques are being used to protect reservoirs from exposure to these elements. The most widely used techniques are stainless steel plating and polymeric coating. In this study, a technique known as arc thermal spraying was used. It is a more convenient and economical method for protecting both concrete and reinforcement steel bar from deterioration in waste water treatment reservoirs. In this study, 316L stainless steel coating was applied to a concrete surface, and different electrochemical experiments were performed to evaluate the performance of coatings in different acidic pH solutions. The coating generated from the arc thermal spraying process significantly protected the concrete surface from corrosion in acidic pH solutions, owing to the formation of a double layer capacitance—a mixture of Cr3+ enriched with Cr2O3 and Cr-hydroxide in inner and Fe3+ oxide on the outer layer of the coating. The formation of this passive film is defective owing to the non-homogeneous 316L stainless steel coating surface. In the pH 5 solution, the growth of a passive film is adequate due to the presence of un-dissociated water molecules in the aqueous sulfuric acid solution. The coated surface is sealed with alkyl epoxide, which acts as a barrier against the penetration of acidic solutions. This coating exhibits higher impedance values among the three studied acidic pH solutions.
We evaluated the applicability of metal spray coating as a waterproofing/corrosion protection method for a concrete structure used for water purification. We carried out an ozone resistance test on four metal sprays and evaluated the water permeability and bond strength of the metals with superior ozone resistance, depending on the surface treatment method. In the ozone resistance test, four metal sprays and an existing ozone-proof paint were considered. In the experiment on the water permeability and bond strength depending on the surface treatment method, the methods of no treatment, surface polishing, and two types of pore sealing agents were considered. The results showed that the sprayed titanium had the best ozone resistance. Applying a pore sealing agent provided the best adhesion performance, of about 3.2 MPa. Applying a pore sealing agent also provided the best waterproofing performance. Scanning electron microscope analysis showed that applying a pore sealing agent resulted in an excellent waterproofing performance because a coating film formed on top of the metal spray coating. Thus, when using a metal spray as waterproofing/corrosion protection for a water treatment concrete structure, applying a pore sealing agent on top of a film formed by spraying titanium was concluded to be the most appropriate method.
Exterior finishes protect reinforced concrete buildings against environmental factors, improve their durability, and enhance their exterior design. In this study, the influence of different metal types used in arc thermal metal spraying on the adhesion between concrete and metal coatings was analyzed. Five metals with different melting points were tested, and the differences between their melting points and surface temperatures immediately after thermal spraying were measured. The bonding strength of each metal was evaluated. Additionally, the interface between the concrete surface and metal coating was analyzed using image analysis and optical microscopy. The results demonstrated that Zn achieved the highest bonding strength (1.84 MPa), which had the lowest melting point and surface temperature immediately after spraying, while Cu/Sn achieved the lowest strength (1.38 MPa), which had the highest temperatures. The bonding strength had a closer relationship (R2 = 0.9946) with the difference between the melting point and surface temperature immediately after spraying than that (R2 = 0.9589) with the surface temperature immediately after spraying. The bonding strength increased as the ratio of the non-interfacial failure area to the total area increased, ensuring a stronger attachment to the concrete surface. Overall, the results showed that the bonding strength was significantly affected by the metal type.
Using a concrete surface, the ingress of aggressive ions and the initiation of the corrosion reaction of an embedded steel rebar were studied. To reduce the corrosion reaction of the embedded steel rebar, either a coating on the steel rebar or a repair material was used on the concrete surface. Therefore, in the present study, 200 µm thick Cu, Ti, and 85Zn-15Al were used as repair materials, and their coatings were deposited on the concrete surface using a twin-wire arc thermal spray process. Different experiments such as bond adhesion, water permeability, immersion in a 5 wt.% NaCl solution, and accelerated carbonation were performed to assess the durability of the coatings, and the characterization of the coatings was performed by using scanning electron microscopy (SEM) and X-ray diffraction (XRD). The Cu and 85Zn-15Al coatings exhibited severe defects and porosity; therefore, these coatings exhibited very low bond adhesion, whereas the Ti coating showed a dense and compact morphology, and its bond adhesion value was 11 times greater than that of the Cu coating. The NaCl immersion results can be used to determine the extent of the deterioration of different coatings in coastal areas; based on these results, the Cu coating exhibited delamination, while 85Zn-15Al showed white rust deposition. By contrast, there was no detrimental effect of NaCl immersion on the Ti coating during the 28 days under study, and the coating exhibited characteristics identical to those observed after deposition. The Ti coating reduced the carbonation depth by 1.5–2 times that of the Cu and 85Zn-15Al coatings after four and eight weeks of exposure. The present study suggests that Ti can be the potential metal used as a repair material for concrete to enhance the durability of buildings and infrastructure.