Regenerated fibers from rennet‐treated casein micelles can be produced with a defined width and homogeneous surface morphology using a two‐substance nozzle integrated in a spinning setup. Extrusion is carried out under standard conditions in a coagulation buffer with 100 × 10−3 m CaCl2 at 60 °C. Electron microscopic images of dried fibers show a fine structure consisting of µm‐sized strands running parallel to the fiber axis and radially outward. Confocal fluorescence microscopy lifetime images show that the strands are rich in free calcium, which is released upon swelling in deionized water and diffuses out of the fiber. Fibers made with only 50 × 10−3 m calcium chloride swell at a higher rate to larger equilibrium swelling values because of fewer stabilizing calcium bridges. In HCl, initial swelling of the fibers is followed by deswelling to a defined equilibrium state with a densely packed casein matrix, as indicated by fluorescence microscopy images. Because of the large number of dissolved calcium contacts and the residual charges on the casein, swelling in HCl occurs very quickly. Elastic contributions of the network and released ions lead to deswelling of the fiber, which occurs fastest for those with 100 × 10−3 m CaCl2 due to the high proportion of free ions.
Regenerated fibers can be prepared from a cooled solution of renneted casein micelles in a wet spinning process. For better handling and stability of the fiber, plasticizers, network modifiers or cross-linkers are used in the production process. For that reason, fibers with different glycerol and calcium content are prepared in this study and subsequently treated with the enzyme transglutaminase before being characterized after air drying. In addition to the swelling behavior in NaOH, H2O, simulated milk ultrafiltrate buffer as well as HCl, the mechanical properties of the fibers are investigated, taking into account their microscopic fine structure. Transglutaminase-treated fibers show sigmoidal absorption curves for all solvents and reach higher equilibrium swelling percentages than untreated fibers. When the calcium content in the coagulation bath is increased from 50 mM to 100 mM, more stabilizing calcium bridges lead to a denser fiber structure that swells more slowly in all solvents considered. With increasing glycerol content, the flexibility of the fibers increases, as indicated by the decrease in elastic moduli, and a fine structure in the sub-µm range becomes visible. The fibers also demonstrate lower elastic moduli when post-treated with transglutaminase. Besides the higher casein content due to the transglutaminase treatment, this could also contribute to the higher equilibrium swelling percentages compared to the untreated fibers.
2 March 2026 in Physical Chemistry Chemical Physics
Differential dynamic microscopy is used to characterize the dynamics of casein micelle dispersions from the dilute to the concentrated regime and to quantitatively probe the aggregation kinetics of para -casein micelles following a temperature jump.