Bulk show a temperature-driven valence transition of europium from above 200 K to below 100 K, which is correlated with a shrinking by approximately 2% of the tetragonal crystal lattice along the two -axes. Due to this interconnection between lattice and electronic degrees of freedom the influence of strain in epitaxial thin films is particularly interesting. Ambient x-ray diffraction (XRD) confirms an epitaxial relationship of tetragonal on MgO(001) with an out-of plane -axis orientation for the thin film, whereby the -axes of both lattices align. XRD at low temperatures reveals a strong coupling of the thin film lattice to the substrate, showing no abrupt compression over the temperature range from 300 to 10 K. Hard x-ray photoelectron spectroscopy at 300 and 20 K reveals a temperature-independent valence of for Eu. The evolving biaxial tensile strain upon cooling is suggested to suppress the valence transition. Instead temperature-dependent transport measurements of the resistivity and the Hall effect in a magnetic field up to 5 T point to a film thickness independent phase transition at 16 to 20 K, indicating magnetic ordering.
Europium intermetallic compounds show a variety of different ground states and anomalous physical properties due to the interactions between the localized 4f electrons and the delocalized electronic states. Europium is also the most reactive of the rare earth metals which might be the reason why very few works are concerned with the properties of Eu-based thin films. Here we address the low-temperature magnetic properties of ferromagnetic EuPd2 thin films prepared by molecular beam epitaxy. The epitaxial (111)-oriented thin films grow on MgO (100) with eight different domain orientations. We analyze the low-temperature magnetic hysteresis behavior by means of micromagnetic simulations taking the multi-domain morphology explicitly into account and quantify the magnetic crystal anisotropy contribution. By ab initio calculations we trace back the microscopic origin of the magnetic anisotropy to thin film-induced uniform biaxial strain.
The material composition and electrical properties of nanostructures obtained from focused electron beam-induced deposition (FEBID) using manganese and vanadium carbonyl precursors have been investigated. The composition of the FEBID deposits has been compared with thin films derived by the thermal decomposition of the same precursors in chemical vapor deposition (CVD). FEBID of V(CO)6 gives access to a material with a V/C ratio of 0.63–0.86, while in CVD a lower carbon content with V/C ratios of 1.1–1.3 is obtained. Microstructural characterization reveals for V-based materials derived from both deposition techniques crystallites of a cubic phase that can be associated with VC1−xOx. In addition, the electrical transport measurements of direct-write VC1−xOx show moderate resistivity values of 0.8–1.2 × 103 µΩ·cm, a negligible influence of contact resistances and signatures of a granular metal in the temperature-dependent conductivity. Mn-based deposits obtained from Mn2(CO)10 contain ~40 at% Mn for FEBID and a slightly higher metal percentage for CVD. Exclusively insulating material has been observed in FEBID deposits as deduced from electrical conductivity measurements. In addition, strong tendencies for postgrowth oxidation have to be considered.
Non-centrosymmetric magnetic materials are a promising platform for stabilizing chiral spin textures, such as skyrmions and cycloidal magnetic states. This is particularly true in epitaxial thin film geometries, where strain and interface effects offer additional control. Herein, we report on the first epitaxial thin films of EuPdSi$_3$ grown by molecular beam epitaxy on MgO(001). X-ray diffraction confirms an epitaxial relationship of tetragonal EuPdSi$_3$ in the BaNiSn$_3$ structure with out-of-plane c-axis orientation and parallel in-plane a-axes. Hard x-ray photoelectron spectroscopy reveals a stable Eu valence of 2.0, yielding a large magnetic moment of approximately 7\,$\upmu_{\text{B}}$ per Eu atom in accordance with Hund’s rule. Owing to the non-centrosymmetric crystal structure, non-collinear magnetic states such as N'{e}el-type skyrmions and cycloidal phases are allowed by symmetry. Electronic transport measurements reveal two magnetic phase transitions at 19\,K and 15\,K in zero applied field. Under magnetic fields applied along the crystallographic [100] and [001] directions, distinct temperature dependent magnetic phases emerge, demonstrating the sensitivity of the magnetic ground state to field orientation in epitaxial EuPdSi$_3$ thin films.
Studying the collective excitations of the spin structure (magnons) in highly ordered materials like epitaxial thin films is an interresting field and offers an insight in the magnertic properties of new materials.Surface Acoustic Waves (SAW) have recently been used to study the phonon-magnon-coupling in for example thin films of Nickel evaporated on piezoelectric substrate material like LiNbO3.More interesting material classes, e.g. valence transition compounds, are usually grown on specially selected substrates to get highly ordered, epitaxial thin films with a specific lattice constant to achieve fine-tuned biaxial tensions which affect the magnetic properties.These substrates are usually non-piezoelectric and the phonon-magnon coupling can't be studied easily. Here we show a procedure that can be used to apply the well established SAW-based methods for the investigation of magnon spectra of epitaxial thin films grown on non-piezoelectric substrates.Using reactive RF sputtering methods, piezoelecxtric thin films can be applied on various non-piezoelectric substrates for the excitation of SAW in these substrates.A carefully coordinated sequence of reactive RF-sputtering, patterning and etching ensures best possible preservation of sensitive thin films.Measurments on well known Nickel thin films are shown as a reference.Further data of more exotic valence transition compounds measured at low temperatures are presented.The presented technique can be adapted by typically equipped thin-film laboratories without further costly investments and thus allows highly-sensitive measurements of the magnon spectrum of thin-film materials in the range of up to ~3 GHz (depending on the quality of available lithography equipment).