View All Publications
20 March 2011 in Oxidation of Metals
Verified
Journal Article
Closed access
PDF file
AAAlina Agüero
Alina Agüero
MOMarcos Gutiérrez del Olmo
Marcos Gutiérrez del Olmo
LKL. Korcakova
L. Korcakova
TNT. T. M. Nguyen
T. T. M. Nguyen
BHB. Hinnemann
B. Hinnemann
SSS. Saadi
S. Saadi

29 September 2024 in Coatings
Verified
Journal Article
Open access
PDF file
AAAlina Agüero
Alina Agüero
PAPauline Audigié
Pauline Audigié
MOMarcos Gutiérrez del Olmo
Marcos Gutiérrez del Olmo
CSCristina Lorente Sánchez
Cristina Lorente Sánchez
JMJulio Mora
Julio Mora
SRSergio Rodríguez
Sergio Rodríguez
The present study focused on demonstrating the versatility of the slurry deposition technique to produce aluminide coatings to protect components from high-temperature corrosion in a broad temperature range, from 400 to 1400 °C. This is a simpler and low-cost coating technology used as an alternative to CVD and pack cementation, which also allows the coating of complex geometries and offers improved and simple repairability for a lot of industrial applications, along with avoiding the use of non-hazardous components. Slurry aluminide coatings from a proprietary water-based-Cr6+ free slurry were produced onto four different substrates: A516 carbon steel, 310H AC austenitic steel, Ti6246 Ti-based alloy and TZM, a Mo-based alloy. The resulting coatings were thoroughly characterised by FESEM and XRD, mainly so that the identification of microstructures and appropriate phases was reported for each coating. The importance of surface preparation and heat treatment as key parameters for the coating final microstructures was also evidenced, and how those parameters can be optimised to obtain stable intermetallic phases rich in Al to sustain the formation of a protective Al2O3 oxide scale. These coating systems have applications in diverse industrial environments in which high-temperature corrosion limits the lifetime of the components.

28 August 2020 in Coatings
Verified
Journal Article
Open access
PDF file
AAAlina Agüero
Alina Agüero
IBIgnacio Baráibar
Ignacio Baráibar
MOMarcos Gutiérrez del Olmo
Marcos Gutiérrez del Olmo
STSatu Tuurna
Satu Tuurna
ATAki Toivonen
Aki Toivonen
PAPertti Auerkari
Pertti Auerkari
The efficiency of ultra-supercritical (USC) steam power plants is limited by the materials properties, in particular, the steam oxidation resistance of the currently used steels at temperatures higher than 600 °C. Under these conditions, steam oxidation results in the development of thick oxide scales which spall and can accumulate in tube bends leading to blockage, overheating and premature creep rupture, as well as erosion of downstream components such as steam valves and turbine blades. Most published work related to oxidation testing is carried out at atmospheric pressure, with significantly less testing of austenitic steels in supercritical steam, and rarely including protective coatings. Indeed, the effect of high-pressure steam in the oxidation process is not quite understood at present. This paper covers a comparison of the behaviour of TP347HFG stainless steel at 700 °C under atmospheric pressure and 25 MPa, with and without slurry-applied diffusion aluminide coatings. The results show a very protective behaviour of the aluminide coatings, which develop a very thin Al-rich protective oxide, and no significant difference between the two environments. In contrast, the uncoated steel exhibited a different behaviour. Indeed, under atmospheric pressure after 3000 h, very thin scales, rich in Cr and not surpassing 5 to 10 µm in thickness, covered the samples along with some much thicker Fe-rich oxide nodules (up to 150 µm). However, under 25 MPa, a thick multilayer scale with a non-homogeneous thickness oscillating between 10 to 120 µm was present. A microstructural investigation was undertaken on the oxidised uncoated and coated substrates. The results suggest that pressure increases the oxidation rate of the chromia former steels but that the oxidation mechanism remains the same. A mechanism is proposed, including early detachment of the outer growing scales under supercritical pressure.

17 October 2024 in ACS Applied Materials & Interfaces
Verified
Journal Article
Open access
AAAlina Agüero
Alina Agüero
PAPauline Audigié
Pauline Audigié
SRSergio Rodríguez
Sergio Rodríguez
MOMarcos Gutiérrez del Olmo
Marcos Gutiérrez del Olmo
JPJon Pascual
Jon Pascual
LJLars-Gunnar Johansson
Lars-Gunnar Johansson
In this work, a slurry iron aluminide-coated ferritic steel SVM12 was subjected to a laboratory experiment mimicking superheater corrosion in a biomass-fired power boiler. The samples were exposed under model Cl-rich biomass conditions, in a KCl + O2 + H2O environment at 600 °C for 168, 2000, and 8000 h. The morphology of corrosion and the composition of the oxide scale and the coating were investigated by a combination of advanced analytical techniques such as FESEM/EDS, SEM/EBSD, and XRD. Even after short-term exposure, the coating developed a very fast-growing and up to 50 μm thick α-Al2O3 scale in contrast to the spontaneous formation of a protective, thin, dense, slow-growing, and very adhesive α-Al2O3 layer usually formed on metallic materials after high-temperature oxidation. In view of the literature on the formation of oxide scales on alloys and coatings, the formation of an α-Al2O3 scale at this relatively low temperature is very surprising in itself. The thick alumina scale was not protective as its formation resulted in fast degradation of the coating and rapid Fe2Al5 → FeAl phase transformation, which in turn generated porosity inside the coating. In all cases, the resulting thick Al2O3 scale was porous and consisted of both equiaxed α-Al2O3 grains and randomly oriented aggregated alumina whiskers. Potassium is concentrated in the outer part of the Al2O3 scale, while chlorine is concentrated close to the scale/aluminide interface. The unexpected formation of rapidly growing α-Al2O3 at relatively low temperature is attributed to the hydrolysis of aluminum chloride generated in the corrosion process.

24 January 2022 in Results in Surfaces and Interfaces
Verified
Journal Article
Open access
AAAlina Agüero
Alina Agüero
MØMaría José Landeira Østergård
María José Landeira Østergård
AHAnette N. Hansson
Anette N. Hansson
MOMarcos Gutiérrez del Olmo
Marcos Gutiérrez del Olmo

12 January 2017 in Oxidation of Metals
Verified
Journal Article
Closed access
PDF file
AAAlina Agüero
Alina Agüero
MOMarcos Gutiérrez del Olmo
Marcos Gutiérrez del Olmo
RMRaúl Muelas
Raúl Muelas