In heterostructures, a still poorly understood phenomenon is that of electron trapping in back-gating experiments. Here, by combining magnetotransport measurements and self-consistent Schrödinger-Poisson calculations, we obtain an empirical relation between the amount of trapped electrons and the gate voltage. The amount of trapped electrons decays exponentially away from the interface. However, contrary to earlier observations, we find that the Fermi level remains well within the quantum well. The enhanced trapping of electrons induced by the gate voltage can therefore not be explained by a thermal escape mechanism. Further gate sweeping experiments strengthen that conclusion. We propose a new mechanism which involves the electromigration and clustering of oxygen vacancies in and argue that such electron trapping is a universal phenomenon in -based two-dimensional electron systems.
17 August 2017 in Physical Chemistry Chemical Physics
Zinc oxide (ZnO) thin films were grown by pulsed layer deposition under an N2 atmosphere at low pressures on a- and r-plane sapphire substrates. Structural studies using X-ray diffraction confirmed that all films had a wurtzite phase. ZnO thin films on a- and r-plane sapphire have grown with orientations along the [0002] and [110] directions, respectively. Room temperature photoluminescence measurements indicate that the presence of native point defects (interstitial zinc, oxygen vacancies, oxygen antisites and zinc vacancies) is more preponderant for ZnO thin films grown on the r-plane sapphire substrate than the sample grown on the a-plane sapphire substrate. Room temperature impedance spectroscopy measurements were performed in an alternating current frequency range from 40 to 105 Hz in the dark and under normal light. An unusual positive photoresistance effect is observed at frequencies above 100 kHz, which we suggest to be due to intrinsic defects present in the ZnO thin films. Furthermore, an analysis of the optical time response revealed that the film grown on the r-plane sapphire substrate responds faster (characteristic relaxation times for τ1, τ2 and τ3 of 0.05, 0.26 and 6.00 min, respectively) than the film grown on the a-plane sapphire substrate (characteristic relaxation times for τ1, τ2 and τ3 of 0.10, 0.73 and 4.02 min, respectively).