Dimensional measurements on nano-objects by atomic force microscopy (AFM) require samples of safely fixed and well individualized particles with a suitable surface-specific particle number on flat and clean substrates. Several known and proven particle preparation methods, i.e., membrane filtration, drying, rinsing, dip coating as well as electrostatic and thermal precipitation, were performed by means of scanning electron microscopy to examine their suitability for preparing samples for dimensional AFM measurements. Different suspensions of nano-objects (with varying material, size and shape) stabilized in aqueous solutions were prepared therefore on different flat substrates. The drop-drying method was found to be the most suitable one for the analysed suspensions, because it does not require expensive dedicated equipment and led to a uniform local distribution of individualized nano-objects. Traceable AFM measurements based on Si and SiO2 coated substrates confirmed the suitability of this technique.
Recently, a novel corrosion-resistant construction material, Carbon Concrete Composite (C3), consisting of coated carbon fibers embedded in a concrete matrix, was introduced. However, thermal exposure during domestic fires may impact the release of organic pollutants and fibers during abrasive processing and/or demolition. Consequently, the objective of this study was to explore the emission characteristics of toxic compounds and harmful fibers during the dry-cutting after exposure to 25–600 °C (3 h, air). These parameters mimic the abrasive machining and dismantling after a domestic fire event. Mass spectrometry and chromatography served as analytical methodologies, and no organic pollutants for exposure temperatures ≥ 400 °C were found. In contrast, significant amounts of pyrolysis products from the organic fiber coating were released at lower temperatures. Studying the morphology of the released fibers by electron microscopy revealed a decrease in fiber diameter for temperatures exceeding 450 °C. At ≥550 °C, harmful fibers, according to the World Health Organization (WHO) definition, occurred (28–41 × 103 WHO fibers/m3 at 550–600 °C). This leads to the conclusion that there is a demand for restraining and protection measures, such as the use of wet cutting processes, suction devices, particle filtering masks and protective clothing, to handle thermally stressed C3.