31 March 2022 in Fullerenes, Nanotubes and Carbon Nanostructures
Verified
Journal Article
Closed access
FLFeng Lu
Feng Lu
THTianen Hao
Tianen Hao
XBXu Bai
Xu Bai
ZFZhengwei Fu
Zhengwei Fu
In order to improve the quality of diamond coatings, this paper combined the chemical etching and buffer layers to deal with cemented carbide with cobalt (Co) content of 8%. Diamond coatings were prepared with hot filament chemical vapor deposition (HFCVD). The surface morphology, quality and wear property were explored by using scanning electron microscopy, X-ray diffraction, laser Raman spectrometer, and friction and wear tester. Compared to the sample with no pretreatment, samples after pretreatment have better surface morphology. There are no obvious impurities as well. Diamond crystals are uniform and compact. Friction and wear test indicated that the friction coefficient is lower than 0.1. Samples after pretreatment are much lower and steady among them. The sample using tungsten(W)-molybdenum(Mo) layer has the best surface morphology and the lowest friction coefficient. The result shows that the pretreatment combined the chemical etching and buffer layers cannot only act as the diffusion barrier, but also can improve the adhesion between substrate and diamond coatings. The effect of composite buffer layer is better than single metal buffer layers.

24 May 2019 in Materials Research Express
Verified
Journal Article
Closed access
PDF file
FLFeng Lu
Feng Lu
HLHui-Xin Li
Hui-Xin Li
LZLi-Qiong Zha
Li-Qiong Zha
YWYi-Bao Wang
Yi-Bao Wang
LLLu-Sheng Liu
Lu-Sheng Liu
ZYZi-Yao Yuan
Zi-Yao Yuan

18 March 2022 in Membranes
Verified
Journal Article
Open access
PDF file
FLFeng Lu
Feng Lu
Tianwei LiuTianwei Liu
Tianwei Liu
XBXu Bai
Xu Bai
YWYuhou Wu
Yuhou Wu
HWHe Wang
He Wang
GYGuangyu Yan
Guangyu Yan
Diamond films were deposited on silicon nitride (Si3N4) substrates with three different roughnesses using the method of hot-filament chemical vapor deposition (HFCVD). The tribological properties of the film were studied by changing the deposition time, deposition distance, and methane (CH4) concentration. The friction coefficient, delamination threshold load, and wear rate of the diamond films were tested and calculated using the reciprocating friction and wear test under dry friction conditions. The results show that, when the deposition time is 12 h, the bonding force of the film is the lowest and the friction coefficient is the largest (0.175, 0.438, and 0.342); the deposition distance has little effect on the friction performance. The friction coefficients (0.064, 0.107, and 0.093) of nano-diamond films (NCD) prepared at a 40 sccm CH4 concentration are smaller than those of micro-diamond films (MCD) prepared at a 16 sccm CH4 concentration. The load thresholds before delamination of Ra 0.4 μm substrate diamond film are as high as 40 N and 80 N, whereas the diamond films deposited on Ra 0.03 μm substrates have lower wear rates (4.68 × 10−4 mm3/mN, 5.34 × 10−4 mm3/mN) and low friction coefficients (0.119, 0.074, 0.175, and 0.064). Within a certain load range, the deposition of a diamond film on a Ra 0.03 μm Si3N4 substrate significantly reduces the friction coefficient and improves wear resistance. Diamond film can improve the friction performance of a workpiece and prolong its service life.

30 December 2010 in Science China Technological Sciences
Verified
Journal Article
Closed access
PDF file
FLFeng Lu
Feng Lu
CXChengHai Xu
ChengHai Xu
LWLiShi Wen
LiShi Wen

16 December 2022 in The International Journal of Advanced Manufacturing Technology
Verified
Journal Article
Closed access
PDF file
FLFeng Lu
Feng Lu
TZTongxiang Zheng
Tongxiang Zheng
XBXu Bai
Xu Bai
YWYuhou Wu
Yuhou Wu
ZFZhengwei Fu
Zhengwei Fu
THTianen Hao
Tianen Hao

1 March 2024 in Materials Research Express
Verified
Journal Article
Open access
XBXu Bai
Xu Bai
XXXiangyang Xue
Xiangyang Xue
FLFeng Lu
Feng Lu
YWYuhou Wu
Yuhou Wu
THTianen Hao
Tianen Hao
Pure MoS2 films exhibit disadvantages such as low densities, poor mechanical properties, and weak wear resistance under atmospheric environments. For this reason, Ti was chosen as the doping element in this work. Mo-S-Ti composite films with different Ti contents were deposited using the magnetron sputtering system, and the effects of Ti content on the chemical composition, mechanical and tribological properties of these films were analyzed by numerous characterization methods to determine the doping content of Ti elements. The results show that the tribological performance of Mo-S-Ti composite film under atmospheric environments reaches the best when the Ti content is 13.48 at%. In addition, the present work also found that longitudinal load and reciprocating frequency have a significant effect on the tribological properties of this film. It is easier to form high quality transfer film on GCr15 balls under higher longitudinal load and lower reciprocating frequency, thus transforming the friction between film and GCr15 ball into the friction between film and transfer film, resulting in excellent tribological performance.