31 March 2022 in Fullerenes, Nanotubes and Carbon Nanostructures
In order to improve the quality of diamond coatings, this paper combined the chemical etching and buffer layers to deal with cemented carbide with cobalt (Co) content of 8%. Diamond coatings were prepared with hot filament chemical vapor deposition (HFCVD). The surface morphology, quality and wear property were explored by using scanning electron microscopy, X-ray diffraction, laser Raman spectrometer, and friction and wear tester. Compared to the sample with no pretreatment, samples after pretreatment have better surface morphology. There are no obvious impurities as well. Diamond crystals are uniform and compact. Friction and wear test indicated that the friction coefficient is lower than 0.1. Samples after pretreatment are much lower and steady among them. The sample using tungsten(W)-molybdenum(Mo) layer has the best surface morphology and the lowest friction coefficient. The result shows that the pretreatment combined the chemical etching and buffer layers cannot only act as the diffusion barrier, but also can improve the adhesion between substrate and diamond coatings. The effect of composite buffer layer is better than single metal buffer layers.
16 December 2022 in The International Journal of Advanced Manufacturing Technology
1 May 2025 in Journal of Materials Engineering and Performance
12 January 2022 in Fullerenes, Nanotubes and Carbon Nanostructures
In this paper, diamond coatings with different microstructure were prepared on cemented carbide substrates by HFCVD technique. The changes of grain growth mode and size of diamond coating under different substrate temperature (800 °C, 850 °C, 900 °C) and carbon source concentration (2%, 4%, 6%) were studied, and the differences of coating performance were explored. Both substrate temperature and carbon source concentration have an effect on grain size. When the grain size is in micron scale (0.5 ∼ 6 μm), the growth mode is columnar crystal competing growth. When the substrate temperature reaches 900 °C and the carbon source concentration is 6%, the diamond grain will be fully secondary nucleated, and the grain size will reduce to the nanometer scale (20 ∼ 50 nm). The growth mode is particle cluster accumulation growth and the rate of growth increases significantly. The increase of grain size will increase the adhesion of the coating and its resistance to wear and external loading. However, it may lead to larger friction coefficient, which is about 0.1. Due to the small grain size, the adhesion force of nanocrystalline diamond coating is obviously smaller than micrystalline diamond coating, but the friction coefficient is only 0.03.