Industrially approved collectors are known to be expensive in the mining sector, which raises production costs. This research shows how three locally manufactured soaps can be used as an alternative for collectors in the flotation process. The chemical composition of the iron oxide sample was determined using X-ray fluorescence (XRF). The soaps were graded according to total fatty matter, free caustic alkali, and lather volume to demonstrate their quality. The iron oxides, which made up 67 % of the total weight, were floated with naphthalene as a frother and locally manufactured soaps, namely Key soap, Alata soap, and Azumah Blow soap, at a collector dosage of 0.6 ml, 1 ml, and 1.4 ml. This was done to establish which soap is the most efficient collector and the dosage that results in the best recovery. Atomic Absorption Spectrometry (AAS) was used to determine the iron content that reported in the feed, concentrates and tailings. Optimum collector dosage was 1 ml, with Alata soap generating the highest recovery of 70.5 %, which compares well with conventional collectors used in iron oxide flotation. The studies also revealed that the total fatty matter, free caustic alkali, and lather volume of locally made soaps have a positive influence on the flotation of iron oxide. However, only Key soap met all the specifications for soaps by the Ghana Standards Authority.
5 December 2024 in Journal of the Ghana Institution of Engineering (JGhIE)
In Ghana, voluminous amounts of slags are generated by fire assay laboratories. Since lead is a major constituent in fire assay slags, it is possible to find its way into the slag matrix and be released into the geo environment upon disposal. This work ascertains the possible amount of lead in the slags and recovers it using flotation, gravity concentration and acid-leaching methods. The initial samples were chemically characterized using an X-ray fluorescence (XRF) and acid-digested for Atomic Absorption Spectroscopy (AAS) analysis. The results indicate that fire assay laboratories have elevated heavy metal concentrations, especially lead (Pb), which is above the Ghana Environmental Protection Agency (GEPA) and World Health Organization (WHO) permissible levels, demonstrating anthropogenic impacts. The study found the recoveries were 77.83 %, 77.09 % and 75.90 % for flotation, gravity separation and acid leaching respectively. It is concluded that the gravity separation method is the best processing route for lead recovery from fire assay slags since the gravity separation poses little or no environmental dangers whereas flotation and acid leaching processes require chemicals that can cause skin irritation and other adverse effects. Also, the gravity separation process requires less time to perform.