This work presents an innovative honeycomb cell geometry design with enhanced in-plane energy absorption under quasi-static lateral loads. Numerical and experimental compression tests results under axial and lateral loads are analyzed. The proposed cell geometry was designed to overcome the limitations posed by standard hexagonal honeycombs, which show relatively low stiffness and energy absorption under loads that have a significant lateral component. To achieve this, the new cell geometry was designed with internal diagonal walls to support the external walls, increasing its stiffness and impact energy absorption in comparison with the hexagonal cell. 3D-printed unit-cell specimens made from ABS thermoplastic material were subjected to experimental quasi-static compression tests, in both lateral and axial directions. Energy absorption was compared to that of the standard hexagonal cell, with the same mass and height. Finite element models were developed and validated using experimental data. Results show that the innovative geometry absorbs approximately 15% more energy under lateral compression, while maintaining the same level of energy absorption of the standard hexagonal cell in the axial direction. The present study demonstrates that the proposed cell geometry has the potential to substitute the standard hexagonal honeycomb in applications where significant lateral loads are present.
Honeycomb cores are widely used in the aerospace and automotive fields as a part of protective structures. Unfortunately, standard prismatic honeycomb cores offer a limited amount of energy absorption under lateral loads and suffer from degradation of their impact-deadening properties when their dimensional scale is increased. In this work, a multiscale study on energy absorption under quasi-static load is carried out on 3D-printed honeycomb core samples constituted by a variable section and compared to the cases of standard hexagonal honeycomb samples having the same mass and external dimensions. When doubling the dimensional scale in the case of lateral loads, the novel core geometry showed a substantial absence of specific energy absorption degradation, whereas the hexagonal core suffered from a 12.2%-degradation. Furthermore, by increasing the dimensional scale, the novel core geometry shows a delay in the densification onset. The variable-core geometry showed an average increase, in terms of energy absorption under lateral loads, of 46.8% for the regular scale and 71.4% for the double scale. Under axial loads, a 12.4%-decrease in energy absorption was observed for the samples with novel geometry, which, nevertheless, showed a relatively constant profile of reaction force under compression: this property could potentially allow it to avoid pre-crushing.