2,6-Di(9H-carbazol-9-yl)pyridine (DiCP) was synthesized and its corresponding homopolymer (PDiCP) and copolymers (P(DiCP-co-CPDT), P(DiCP-co-CPDT2), P(DiCP-co-CPDTK), and P(DiCP-co-CPDTK2)) were synthesized electrochemically. The anodic copolymer with DiCP:cyclopentadithiophene ketone (CPDTK) = 1:1 feed molar ratio showed high transmittance change (ΔT%) and colouration efficiency (η), which were measured as 39.5% and 184.1 cm2 C−1 at 1037 nm, respectively. Electrochromic devices (ECDs) were composed of PDiCP, P(DiCP-co-CPDT), P(DiCP-co-CPDT2), P(DiCP-co-CPDTK), and P(DiCP-co-CPDTK2) as anodically-colouring polymers, and poly(3,4-ethylenedioxythiophene)-poly(styrene sulfonic acid) (PEDOT-PSS) as cathodically-colouring polymers. P(DiCP-co-CPDTK)/PEDOT-PSS ECD showed light silverish-yellow at 0.0 V, light grey at 0.7 V, grey at 1.3 V, light greyish blue at 1.7 V, and greyish blue at 2.0 V. Moreover, P(DiCP-co-CPDTK)/PEDOT-PSS ECD presented high ΔT (38.2%) and high η (633.8 cm2 C−1) at 635 nm.
A series of carbazole-based polymers (PdCz, P(dCz2-co-dTC1), P(dCz2-co-dTC2), P(dCz1-co-dTC2), and PdTC) were deposited on indium tin oxide (ITO) conductive electrodes using electrochemical polymerization. The as-prepared P(dCz2-co-dTC2) displayed a high ΔT (57.0%) and multichromic behaviors ranging from yellowish green, greenish gray, gray to purplish gray in different redox states. Five organic electrochromic devices (ECDs) were built using dCz- and dTC-containing homopolymers and copolymers as anodic materials, and poly(3,4-(2,2-dimethylpropylenedioxy)thiophene) (PProdot-Me2) as the cathodic material. The P(dCz2-co-dTC2)/PProdot-Me2 ECD presented remarkable electrochromic behaviors from the bleached to colored states. Moreover, P(dCz2-co-dTC2)/PProdot-Me2 ECD displayed a high optical contrast (ΔT, 45.8%), short switching time (ca. 0.3 s), high coloration efficiency (528.8 cm2 C−1) at 580 nm, and high redox cycling stability.
The green blends of an ionic liquid, 1-ethyl-3-propylimidazolium bis(trifluoromethanesulfonyl)imide {[EPrI][TFSI]}, and a biodegradable polymer, poly(3-hydroxybutyrate) (PHB), were investigated in this study. The influence of an ionic liquid on the crystallization behaviors of a biodegradable polymer was explored. In the blends, the presence of [EPrI][TFSI] decreased the Tg and Tm of PHB. Incorporating [EPrI][TFSI] in the blends reduced the degree of crystallinity of PHB, inferring that the [EPrI][TFSI] weakened the crystallization of PHB. It further showed retarded isothermal and non-isothermal crystallization for PHB with the presence of [EPrI][TFSI]. The smaller K and 1/t0.5 estimated by the Avrami equation for the blends indicated that [EPrI][TFSI] weakened the isothermal crystallization of PHB with exhibiting the slower crystallization rate. The present study also discussed non-isothermal crystallization of the blends. We found that the Mo model, which is generally used to discuss the non-isothermal crystallization, adequately described the non-isothermal behaviors of the [EPrI][TFSI]/PHB blends. By increasing the [EPrI][TFSI] content, the rate-related parameter F(T) systematically increased, inferring a decreased crystallization rate of PHB with the addition of [EPrI][TFSI] in the blends. The FTIR results suggested an ion–dipole interaction between [EPrI][TFSI] and PHB. This proposes the occurrence of possible complexation between [EPrI][TFSI] and PHB.
Applications of cellulose nanofibers currently match the demands of biodegradable and renewable constituent biocomposites. In this study, we studied the process of preparing TEMPO-oxidized cellulose nanofibers (TOCNs). These nano-sized cellulose fibers (ca. 11 nm) can be fabricated to high transmittance and optically transparent paper (OP) films. Then the OP films can be facilely immobilized initiating sites for the subsequent surface-initiated atom transfer radical polymerization (SI ATRP). We investigated SI ATRP with styrene (St) kinetics and monitored chemical structure changes of the OP surfaces. The obtained OP-g-PSt significantly led to enhance thermal stability and alter the OP surface with hydrophobic compared to that of pristine OP film. Characterization was studied by Fourier transform infrared spectroscopy (FT-IR), powder X-ray diffraction (XRD), X-ray photoelectron spectroscopy (XPS), scanning electron microscopy (SEM), UV–Vis spectroscopy, thermogravimetric analyzer (TGA), and water contact angle (WCA) measurements.