In this work, we studied the phases in a Mg-Ti-O system using a 1:1 formulation of MgO:TiO2, mixing synthetic brucite of Mexican origin with TiO2 microparticles of high purity, with a heat treatment at 1100 °C for 1 h. Due to its valence electrons, TiO2 can contribute to the sintering process to improve density in MgO products. The raw materials and formulation by XPS and X-RD techniques were characterized. The results demonstrate the presence of different oxidation states in titania and the formation of different oxides in the Mg-Ti-O system when mixed and calcined at 1100 °C; additionally, we estimated the formation of vacancies in the crystal lattice during the transformation from hexagonal brucite to magnesia with a cubic structure centered on the faces. Its thermal behavior is indicated by the MgO-TiO2 phase diagram.
In this paper, the phases in the Mg-Ti-O system using the 1:1 formulation of MgO:TiO2 mixing synthetic brucite of Mexican origin with TiO2 microparticles of high purity and with a heat treatment at 1100°C for 1 h were studied. The raw materials and formulation by XPS and DRX techniques were characterized. The results demonstrate the presence of different oxidation states in titania and the formation of different oxides in the Mg-Ti-O system when mixed and calcined at 1100°C; additionally, the formation of vacancies in the crystal lattice during the transformation from hexagonal brucite to magnesia with a cubic structure centered on the faces is estimated. With the results, its thermal behavior is warned based on the MgO-TiO2 phase diagram.