The S phase, known as expanded austenite, is formed on the surfaces of austenitic stainless steels that are nitrided under low temperature plasma. A similar phase was observed for nitrided ferritic stainless steels and was designed as expanded ferrite or ferritic S phase. The authors treated samples of austenitic AISI 304L and AISI 316L and ferritic AISI 409 stainless steels by plasma nitriding at different temperatures and then studied the structural, morphological, chemical and corrosion characteristics of the modified layers by X-ray diffraction, scanning electron microscopy/energy dispersive spectroscopy and electrochemical tests. For both austenitic AISI 304L and AISI 316L stainless steels, the results showed that a hard S phase layer was formed on the surfaces, promoting an anodic polarisation curve displacement to higher current density values that depend on the plasma nitriding temperature. A layer having a high amount of nitrogen was formed on the ferritic AISI 409 stainless steel. X-ray diffraction measurements indicated high strain states for the modified layers formed on the three stainless steels, being more pronounced for the ferritic S phase.
26 October 2009 in Journal of Applied Polymer Science
This paper describes an investigation on CuO and CuO-ZnO catalysts supported on CeO(2) and CeO(2)-La(2)O(3) oxides, which were designed for the low temperature water-gas shift reaction (WGSR). Bulk catalysts were prepared by co-precipitation of metal nitrates and characterized by energy-dispersive spectroscopy (EDS), X-ray diffraction (XRD), surface area (by the BET method), X-ray photoelectron spectroscopy (XPS), and in situ X-ray absorption near edge structure (XANES). The catalysts` activities were tested in the forward WGSR, and the CuO/CeO(2) catalyst presented the best catalytic performance. The reasons for this are twofold: (1) the presence of Zn inhibits the interaction between Cu and Ce ions, and (2) lanthanum oxide forms a solid solution with cerium oxide, which will cause a decrease in the surface area of the catalysts. Also the CuO/CeO(2) catalyst presented the highest Cu content on the surface, which could influence its catalytic behavior. Additionally, the Cu and Cu(1+) species could influence the catalytic activity via a reduction-oxidation mechanism, corroborating to the best catalytic performance of the Cu/Ce catalyst. (c) 2010 Elsevier B.V. All rights reserved.Brazilian agency FAPESPFundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)Brazilian agency CNP