The electrical contact of the source and drain regions in state-of-the-art CMOS transistors is nowadays facilitated through NiSi, which is often alloyed with Pt in order to avoid morphological agglomeration of the silicide film. However, the solid-state reaction between as-deposited Ni and the Si substrate exhibits a peculiar change for as-deposited Ni films thinner than a critical thickness of tc = 5 nm. Whereas thicker films form polycrystalline NiSi upon annealing above , thinner films form epitaxial NiSi2 films that exhibit a high resistance toward agglomeration. For industrial applications, it is therefore of utmost importance to assess the critical thickness with high certainty and find novel methodologies to either increase or decrease its value, depending on the aimed silicide formation. This paper investigates Ni films between 0 and 15 nm initial thickness by use of “thickness gradients,” which provide semi-continuous information on silicide formation and stability as a function of as-deposited layer thickness. The alloying of these Ni layers with 10% Al, Co, Ge, Pd, or Pt renders a significant change in the phase sequence as a function of thickness and dependent on the alloying element. The addition of these ternary impurities therefore changes the critical thickness tc. The results are discussed in the framework of classical nucleation theory.
The effect of thermal annealing on epitaxial GeSn (6.5% Sn) strained layers grown on Ge-buffered Si(100) wafers has been investigated using Rutherford backscattering spectrometry and X-ray diffraction to unambiguously determine the Sn substitutional content as well as the elastic strain in the layers. Vacuum annealing at temperatures below 400 °C for 20 min has no noticeable effect on the strain in the epitaxial layers. Once the temperature was raised above 400 °C, however, relaxation of the layer sets in and the GeSn layer has essentially completely relaxed following a 20 min anneal at 650 °C. Using Rutherford backscattering and channelling spectrometry to provide compositional information as a function of depth enables one to monitor the effect of the thermal anneal on the Sn distribution throughout the layer, and also to directly extract their substitutional fraction (i.e., their solubility in the lattice). The results obtained show that when the relaxation initially sets in both the Ge and the Sn remain firmly bound in substitutional lattice sites and it is only around 600 °C, and after substantial relaxation has taken place, that Sn is finally expelled from lattice sites and diffuses to the surface of the sample.
We studied the solid-phase reaction between a thin Ni film and a single crystal Ge(001) or Ge(111) substrate during a ramp anneal. The phase formation sequence was determined using in situ X-ray diffraction and in situ Rutherford backscattering spectrometry (RBS), while the nature and the texture of the phases were studied using X-ray pole figures and transmission electron microscopy. The phase sequence is characterized by the formation of a single transient phase before NiGe forms as the final and stable phase. X-ray pole figures were used to unambiguously identify the transient phase as the ϵ-phase, a non-stoichiometric Ni-rich germanide with a hexagonal crystal structure that can exist for Ge concentrations between 34% and 48% and which forms with a different epitaxial texture on both substrate orientations. The complementary information gained from both RBS and X-ray pole figure measurements revealed a simultaneous growth of both the ϵ-phase and NiGe over a small temperature window on both substrate orientations.
5 February 2019 in Journal of Physics D: Applied Physics
Solid-state amorphization, the growth of an amorphous phase during annealing, has been studied in a wide variety of thin film structures. Whereas research on the remarkable growth of such a metastable phase has mostly focused on strictly binary systems, far less is known about the influence of impurities on such reactions. In this paper, the influence of nitrogen, introduced via ion implantation, is studied on the solid-state amorphization reaction of thin (35 nm) Ni films with Si, using in situ x-ray diffraction (XRD), ex situ Rutherford backscattering spectrometry, XTEM, and synchrotron XRD. It is shown that due to small amounts of nitrogen (<2 at.%), an amorphous Ni–Si phase grows almost an order of magnitude thicker during annealing than for unimplanted samples. Nitrogen hinders the nucleation of the first crystalline phases, leading to a new reaction path: the formation of the metal-rich crystalline silicides is suppressed in favour of an amorphous Ni–Si alloy; during a brief temperature window between 330 and 350 °C, the entire film is converted to an amorphous phase. The first crystalline structure to grow is the orthorhombic NiSi phase. We demonstrate that this impurity-enchanced solid-state amorphization reaction occurs only under specific implantation conditions. In particular, the initial distribution of nitrogen upon implantation is crucial: sufficient nitrogen impurities must be present at the interface throughout the reaction. Introducing implantation damage without nitrogen impurities (e.g. by implanting a noble gas) does not cause the enhanced solid-state amorphization reaction. Moreover, we show that the stabilizing effect of nitrogen on amorphous Ni–Si films (with a composition ranging from 40% to 50% Si) is not restricted to thin film reactions, but is a general feature of the Ni–Si system.