Most textile waste is either incinerated or landfilled today, yet, the material could instead be recycled through chemical recycling to new high-quality textiles. A first important step is separation since chemical recycling of textiles requires pure streams. The focus of this paper is on the separation of cotton and PET (poly(ethylene terephthalate), polyester) from mixed textiles, so called polycotton. Polycotton is one of the most common materials in service textiles used in sheets and towels at hospitals and hotels. A straightforward process using 5–15 wt% NaOH in water and temperature in the range between 70 and 90 °C for the hydrolysis of PET was evaluated on the lab-scale. In the process, the PET was degraded to terephthalic acid (TPA) and ethylene glycol (EG). Three product streams were generated from the process. First is the cotton; second, the TPA; and, third, the filtrate containing EG and the process chemicals. The end products and the extent of PET degradation were characterized using light microscopy, UV-spectroscopy, and ATR FT-IR spectroscopy, as well as solution and solid-state NMR spectroscopy. Furthermore, the cotton cellulose degradation was evaluated by analyzing the intrinsic viscosity of the cotton cellulose. The findings show that with the addition of a phase transfer catalyst (benzyltributylammonium chloride (BTBAC)), PET hydrolysis in 10% NaOH solution at 90 °C can be completed within 40 min. Analysis of the degraded PET with NMR spectroscopy showed that no contaminants remained in the recovered TPA, and that the filtrate mainly contained EG and BTBAC (when added). The yield of the cotton cellulose was high, up to 97%, depending on how long the samples were treated. The findings also showed that the separation can be performed without the phase transfer catalyst; however, this requires longer treatment times, which results in more cellulose degradation.
Material recycling requires solutions that are technically, as well as economically and ecologically, viable. In this work, the technical feasibility to separate textile blends of viscose and polyester using alkaline hydrolysis is demonstrated. Polyester is depolymerized into the monomer terephthalic acid at high yields, while viscose is recovered in a polymeric form. After the alkaline treatment, the intrinsic viscosity of cellulose is decreased by up to 35%, which means it may not be suitable for conventional fiber-to-fiber recycling; however, it might be attractive in other technologies, such as emerging fiber processes, or as raw material for sugar platforms. Further, we present an upscaled industrial process layout, which is used to pinpoint the areas of the proposed process that require further optimization. The NaOH economy is identified as the key to an economically viable process, and several recommendations are given to decrease the consumption of NaOH. To further enhance the ecological end economic feasibility of the process, an increased hydrolysis rate and integration with a pulp mill are suggested.
Chemical recycling of textiles holds the potential to yield materials of equal quality and value as products from virgin feedstock. Selective depolymerization of textile polyester (PET) from regenerated cellulose/PET blends, by means of alkaline hydrolysis, renders the monomers of PET while cellulose remains in fiber form. Here, we present the mechanism and reactivity of textile PET during alkaline hydrolysis. Part I of this article series focuses on the cellulose part and a possible industrialization of such a process. The kinetics and reaction mechanism for alkaline hydrolysis of polyester packaging materials or virgin bulk polyester are well described in the scientific literature; however, information on depolymerization of PET from textiles is sparse. We find that the reaction rate of hydrolysis is not affected by disintegrating the fabric to increase its surface area. We ascribe this to the yarn structure, where texturing and a low density assures a high accessibility even without disintegration. The reaction, similar to bulk polyester, is shown to be surface specific and proceeds via endwise peeling. Finally, we show that the reaction product terephthalic acid is pure and obtained in high yields.
11 October 2018 in Journal of Materials Chemistry C
High-voltage direct-current (HVDC) cables are a critical component of tomorrow's power grids that seamlessly integrate renewable sources of energy. The most advanced power cable technology uses crosslinked polyethylene (XLPE) insulation, which is produced by peroxide crosslinking of low-density polyethylene (LDPE). Peroxide crosslinking gives rise to hazardous byproducts that compromise the initially excellent purity and cleanliness of LDPE, and hence increase the electrical conductivity of the insulation material. Therefore, a byproduct-free curing process, which maintains the processing advantages and high electrical resistivity of LDPE, is in high demand. Here, we demonstrate a viable alternative to peroxide crosslinking that fulfils these requirements. Click chemistry reactions between two polyethylene copolymers allow the design of a curing process that is additive-free and does not result in the release of any byproducts. The thermoplastic copolymer blend offers a broad processing window up to 140 °C, where compounding and shaping can be carried out without curing. At more elevated temperatures, epoxy and acrylic acid functional groups rapidly react without byproduct formation to form an infusible network. Strikingly, the crosslinked copolymer blend exhibits a very low direct-current (DC) electrical conductivity of 2 × 10−16 S cm−1 at a typical cable operating temperature of 70 °C, which is on par with values measured for both ultra-clean LDPE and commercial XLPE. Hence, the use of polyethylene copolymer blends opens up the possibility to replace peroxide crosslinking with click chemistry type reactions, which may considerably expand the versatility of the most common type of plastic used today.