Traditional solid nanoparticle aerogels have been unable to meet the requirements of practical application due to their inherent brittleness and poor infrared shielding performance. Herein, combining vacuum impregnation and high-temperature pyrolysis, a novel micro/nano-composite fibrous aerogel was prepared via in situ synthesis of silicon carbide nanowires (SiC NWS) in mullite fiber (MF) preform. During this process, uniformly distributed SiC NWS in the MF preform serve as an enhancement phase and also act as an infrared shielding agent to reduce radiation heat transfer, which can significantly improve the mechanical properties of the mullite fiber/silicon carbide nanowire composite aerogels (MF/SiC NWS). The fabricated MF/SiC NWS exhibited excellent thermal stability (1400 °C), high compressive strength (~0.47 MPa), and outstanding infrared shielding performance (infrared transmittance reduced by ~70%). These superior properties make them appealing for their potential in practical application as high-temperature thermal insulators.
1 February 2026 in Journal of Physics: Conference Series
In this paper, we propose a method for rapidly preparing alumina fibre-reinforced silica ceramic matrix (Al 2 O 3f /SiO 2 ) composites. This method involves four cycles of vacuum impregnation, sol-gel, and high-temperature sintering, using silica sol and alumina fibre as raw materials. The mechanical and dielectric properties of the composites were subjected to a systematic examination and characterisation. The results suggest that when the preparation temperature is set to 1000 °C, the prepared Al 2 O 3f /SiO 2 composites may exhibit the best mechanical properties. We are pleased to report that the specific performance of the material is as follows: flexural strength at room temperature reaches 129.84 MPa, tensile strength is 98.87 MPa, interlaminar shear strength is 13.38 MPa, and compressive strength is 122.20 MPa. At 1200 °C, the composite displays an encouraging retention rate of over 80% in high-temperature mechanical strength, which is a promising indication of its potential for high-temperature resistance. Furthermore, the Al 2 O 3f /SiO 2 composite displays a stable and low dielectric constant in the temperature range from room temperature to 1000 °C at 10 GHz, which is between 3.80 and 4.09. This suggests that the material may possess excellent dielectric properties in a high-temperature environment. It is hoped that this study will prove to be a valuable reference point for the preparation of Al 2 O 3f /SiO 2 composites and their potential applications in extreme conditions.