In order to investigate the optimization of the performance and structure of a tungsten crucible CVD reactor, the CFD simulation method was used in this paper to simulate the internal flow of the tungsten crucible CVD reactor. The velocity distribution and temperature distribution in the reactor were obtained. The simulation results show that the axial and radial heat convection will occur between the susceptor and the outer wall surface, but the axial heat convection is more intense. Moreover, it was found that the temperature distribution in the CVD reactor was more uniform and reasonable when the upper gas inlet was applied, which was beneficial to the reduction and deposition processes of tungsten. The molar ratio of H2 to WF6 has a great influence on the deposition rate of tungsten, and excess H2 is not conducive to the deposition of tungsten. Thermal radiation has a great influence on the temperature distribution of CVD reactors. It cannot be neglected.
Conventional powder metallurgy techniques fail to meet the demands for ultrahigh purity tungsten (UHPW) and scalable component sizes required by the semiconductor industry. In this study, ultrahigh purity (99.999998 wt %) large-size tungsten parts, with an adjustable thickness and a diameter of 350 mm, were prepared via a chemical vapor deposition (CVD) method using ultrahigh purity (99.9999 wt %) tungsten hexafluoride (WF6) as the precursor. The microstructure and physical properties of the resulting CVD-UHPW were evaluated and compared with those of powder metallurgy tungsten (PM-W). The results indicate that CVD-UHPW displays a columnar grain microstructure with a lower dislocation density and internal strain, whereas PM-W shows an equiaxed grain microstructure. CVD-UHPW has a density of 19.17 g/cm3, closely matching the theoretical density of tungsten (19.35 g/cm3) and significantly higher than PM-W's density of 18.79 g/cm3. The specific heat capacities of CVD-UHPW, measured from 298 to 1473 K, range from 0.113 to 0.146 J/g·K, similar to PM-W's range of 0.120 to 0.151 J/g·K. CVD-UHPW shows improved electrical and thermal conductivities compared to PM-W, with values ranging from 1.68 × 106 to 1.78 × 107 S/m and 105.7 to 196.4 W/(m·K) from 298 to 1473 K. This study highlights the potential of the CVD method for the large-scale production of ultrahigh purity tungsten parts, emphasizing its significant applicability across various industries.