Mold with diameter sizes of 140 mm, 80 mm, 40 mm and 15 mm were designed to obtain the ingot of Fe-30Mn-10Al-1.1C low-density steel under different cooling rates. The influence of cooling rate on the grain morphology and elemental segregation behavior during the steel solidification process was analyzed by methods including inductively coupled plasma, scanning electron microscope and energy dispersive spectroscopy. The solidification sequence of the low-density steel was calculated by JMatPro 7.0 thermodynamic software. The results show that the microstructure of the steel is mainly austenite and contains a small amount of ferrite. The solidification order in the steel is: L → α, L → γ and α → γ, L → γ + MC. As the cooling rate increases from 1.69 °C/s to 10.28 °C/s, the ferrite phase precipitation increases by 16.7%, and the grain size decreases significantly, and in particular, the austenitic grain size decreases by 26%. With the increase in cooling rate, the microscopic segregation value of aluminum decreases approximately to 1. Additionally, the microscopic segregation of manganese showed a trend of increasing first and then decreasing. Microscopic segregation of Al and Mn can be improved significantly by increasing the cooling rate.
The continuous casting of Ti-Nb microalloyed steel was simulated with high temperature confocal laser scanning microscopy (HTCLSM). Evolution of the sample surface morphology was observed in-situ, during cooling conditions chosen to represent different locations in a cast slab. Calculations with a thermodynamics model of carbonitride precipitate formation agreed with the transmission electron microscopy (TEM) analysis that fine reliefs observed on the sample surface were actually caused by interior precipitation of (Ti,Nb)(C,N). Precipitation and the resulting reliefs changed with location beneath the slab surface, simulated casting speed, and steel composition. With the same casting speed and steel composition, reliefs in the simulated slab surface sample appeared earlier and were larger than in the slab center. With increased casting speed, reliefs were observed later and decreased in size. With increased titanium or niobium content, reliefs appeared earlier and increased in number. TEM measurement showed that the precipitate diameters were mainly smaller than 4 nm, with a few between 4 and 8 nm. The property of surface reliefs observed via HTCLSM correlated qualitatively with the number and size of internal precipitates measured with TEM, showing this to be an effective tool for indirectly characterizing nanoscale secondary phase precipitation inside the sample.