This work is focused on optimising a low-temperature delignification as holocellulose purification pretreatment of Platanus acerifolia leaf waste for second-bioethanol production. Delignification was accomplished by acid-oxidative digestion using green reagents: acetic acid and 30% hydrogen peroxide 1:1. The effect of reaction time (30–90 min), temperature (60–90 °C), and solid loading (5–15 g solid/20 g liquid) on delignification and solid fraction yield were studied. The process parameters were optimised using the Box–Behnken experimental design. The highest attained lignin removal efficiency was larger than 80%. The optimised conditions of delignification, while maximising holocellulose yield, pointed to using the minimum temperature of the examined range. Analysis of variance on the solid fraction yield and the lignin removal suggested a linear model with a negative influence of the temperature on the yield. Furthermore, a negative effect of the solid loading and low effect of temperature and time was found on the degree of delignification. Then the temperature range was extended back to 60 °C, providing 71% holocellulose yield and 70% while improving energy efficiency by working at a lower temperature. Successful lignin removal was confirmed using confocal laser scanning microscopy. As evaluated by scanning electron microscopy, the solid structure presented an increased exposition of the cellulose fibre structure.
Hydrodynamic cavitation (HC) has emerged as a versatile method for modifying the rheological properties of polymer solutions, offering advantages such as scalability and operational simplicity. This work investigates the effect of HC on aqueous polyacrylamide (PAM) solutions, focusing on viscosity and viscoelasticity changes as a function of the number of passes through a vortex-type HC device and the presence of dissolved salts (CaCl2 or KCl). Viscosity measurements were modeled using the power law equation, while oscillatory tests were used to determine storage and loss moduli. The results show that HC substantially reduced viscosity and elastic behavior, with the degree of modification strongly influenced by the number of passes. A critical molecular size limit was suggested, below which further degradation becomes limited. Salt addition enhanced depolymerization, likely due to charge screening, hydrodynamic radius reduction, and the increased solubility and mobility of polymer chains within cavitation bubbles. HC eliminated elasticity in all cases, yielding solutions with near-Newtonian behavior. The transformation is attributed to molecular weight reduction and changes in molecular size distribution. These findings support the use of HC as a practical approach to tailor the flow properties of PAM solutions, while highlighting intrinsic limitations imposed by cavitation dynamics and polymer chain dimensions.
Lignocellulosic biomass is a promising renewable resource for sustainable biorefineries, although its commercial use remains limited by the complex biomass structure and process inefficiencies. This work investigates the use of hydrodynamic cavitation (HC) as a process-intensification strategy during the washing step following hydrogen peroxide–acetic acid (HPAC) delignification, with the aim of enhancing subsequent enzymatic saccharification to produce glucose. Wood residues from Eucalyptus sp., Tipuana tipu, and Pinus sp. were delignified using HPAC under mild conditions (1:1 v/v glacial acetic acid: 30% w/w H2O2 solutions, at 90 °C, 15 g/L, 1 h orbital shake) and washed either by conventional soaking or by HC-assisted recirculation prior to enzymatic hydrolysis using the Novozymes Cellic CTec3 blend at optimal initial conditions (40 FPU/g substrate, pH = 5, and 53 °C). HC applied during washing significantly increased glucose yields and initial hydrolysis rates for delignified angiosperm species. Glucose yields after 28 h increased significantly for Eucalyptus sp. and Tipuana tipu compared to conventional washing, while little effect was found for Pinus sp. Overall, the glucose yield, expressed per 100 g of precursor dry mass, attained 34.5 g/100 g for Eucalyptus sp., 30.2 g/100 g for Tipuana tipu, and only 12.9 g/100 g for Pinus sp. Structural and morphological analyses indicate that the effectiveness of HC is species-dependent and might be associated with fiber disruption and the removal of inhibitory compounds rather than changes in cellulose crystallinity. Implementing HC during the washing step involved 7% extra energy compared to the energy required for HPAC, thus resulting in less energy required per unit mass of glucose generated. These results demonstrate that HC-assisted washing is an effective and energy-efficient intensification step when combined with HPAC, contributing to improved biomass valorization while avoiding harsher pretreatment conditions. Since HC is relatively simple to scale up, the proposed strategy offers an energy-convenient approach for enhancing enzymatic saccharification in sustainable biorefinery processes.