Multiple compression tests on rock-like samples of pre-existing cracks with different geometries were conducted to investigate the strength properties and crack propagation behavior considering multi-crack interactions. The progressive failure process of the specimens was segmented into four categories and seven coalescence modes were identified due to different crack propagation mechanisms. Ultimately, a mechanical model of the multi-crack rock mass was proposed to investigate the gradual fracture and damage evolution traits of the multi-crack rock on the basis of exploring the law of the compression-shear wing crack initiation and propagation. A comparison between theory and experimental results indicated that the peak strength of the specimens with multiple fractures decreased initially and subsequently increased with the increase in the fissure inclination angles; the peak strength of specimens decreased with the increase in the density of fissure distribution.
According to fracture mechanics theory, the initial cracking law and wing crack propagation model of compression shear rock cracks subjected to hydraulic pressure and far field stresses are discussed. The results of the theoretical study show that crack initiation strength is inversely related to hydraulic pressure, that hydraulic pressure aggravates the wing crack’s growth, and that the wing crack’s behavior under high hydraulic pressure shifts from stable to unstable expansion. The confining pressure is proportional to the rock mass strength, the wing crack’s stress intensity factor drops as the remote field stress increases, and the wing crack tends to expand stably. As the crack angle increases, the cracking strength reduces at first, then increases. At the same time, damage fracture mechanics models are established for the occurrence of wing crack-wing crack failure, wing crack-shear crack failure, wing crack-shear crack-wing crack failure, and shear crack-shear crack failure in the compression-shear crack bridge under far-field stress and hydraulic pressure. The link between hydraulic pressure, confining pressure, fracture angle, stress intensity factor, and compression-shear factor is also clarified. The value of the stress intensity factor increases when the hydraulic pressure decreases, the confining pressure increases, and the crack angle increases, whereas the compression-shear factor decreases. This study lays the groundwork for a quantitative assessment of fractured rock mass destruction under hydraulic pressure.
Indoor direct shear tests under different stress levels were conducted on sandstone–concrete samples to investigate the rock–concrete interfaces’ shear energy evolution features and fracture behaviors under different normal stresses, combined with acoustic emission (AE) and digital image correlation (DIC) techniques. The research results show that the growth of normal stress restricts the coalescence and failure of micro-cracks inside the sample and improves the bearing capacity. The shear strength of the sandstone–concrete cemented interface increases by 12.3–34.34% with increasing normal stress. The evolution behaviors of the total input energy, elastic strain energy and dissipated energy density are similar under different normal stress conditions, and the increase in normal stress raises the energy storage capacity of the sample, as well as the input external energy required for a sample’s failure, thereby enhancing the bearing capability of the sample. In addition, the AE count and b value characteristics indicate that crack propagation shows a three-stage variation trend. It can be seen from the RA (rise time/amplitude)-AF (AE count/duration time) curves that as the normal stress increases, the proportion of shear cracks in the sample progressively increases. When the final overall failure of the sample is imminent, the high-energy level fracture type changes from tensile fracture to shear fracture with increased normal stress, leading to an increasing percentage of shear fracture. Finally, the speckle results indicate that the nucleation and coalescence of tensile wing-shaped cracks are the main causes of sample failure. Under relatively high normal stress conditions, the damage degree of the serrated interface increases and the crack morphology becomes more intricate.
In high-elevation mining areas, the roadbeds of certain surface ore haul roads are predominantly composed of sandstone. These sandstones are exposed to cold climatic conditions for long periods and are highly susceptible to erosion by the effects of freeze–thaw, which can degrade their support properties. This paper investigates the mechanism of strength deterioration of sandstone containing prefabricated cracks under cyclic loading and unloading after experiencing freeze–thaw. Sandstone specimens containing prefabricated cracks were prepared and subjected to 0, 20, 40, 60, and 80 freeze–thaw cycle tests. The strength changes were tested, and the crack extension process was analyzed using numerical simulation techniques. The study results show the following: 1. The wave propagation speed within the sandstone is more sensitive to changes in the number of freeze–thaw cycles. In contrast, mass damage shows significant changes only when more freeze–thaw cycles are experienced. 2. As the number of freeze–thaw cycles increases, the frequency of energy release from the numerical model accelerates. 3. The trend of the Cumulative Strain Difference () reflects that the plastic strain difference between numerical simulation and actual measurement gradually decreases with increasing stress cycle level. 4. With the increase in freeze–thaw cycles, the damage morphology of the specimen undergoes a noticeable change, which is gradually transformed from monoclinic shear damage to X-shaped conjugate surface shear damage. 5. The number of tensile cracks dominated throughout the cyclic loading and unloading process, but with the increase in freeze–thaw cycles, the percentage of shear cracks increased. As the freeze–thaw cycles increase, sandstones are more inclined to undergo shear damage. These findings are important guidelines for road design and maintenance in alpine mining areas.
Acoustic emission (AE) and digital image correlation (DIC) techniques enable real-time capture of damage signals and full-field deformation at anchored rock–concrete interfaces under shear loading, which is critical for quantitatively characterizing freeze–thaw (F-T) degradation and preventing geological disasters in cold regions. This study synchronously monitored full-shear-process AE signals using a broadband AE system (150 kHz resonant frequency, 5 MS/s sampling) and captured high-precision full-field deformation via a 5-megapixel monocular DIC system (25 fps). F-T cycle and direct shear tests were conducted on sandstone–concrete anchored specimens with varying F-T cycles and anchor depths to investigate their effects on shear mechanical properties, AE characteristics and failure modes. Results show that AE peak ring count first decreases by 44.9% then increases by 56.5%, while cumulative ring count exhibits a three-stage evolution. Shear crack proportion first decreases then increases, with tensile failure remaining dominant throughout. DIC reveals that F-T cycles shift failure from crack propagation to surface delamination and interface slip, while different anchor depths induce distinct failure patterns. This study confirms that AE and DIC can accurately characterize F-T degradation, providing a reliable non-destructive monitoring method for cold-region anchorage engineering.