-quartz-type solid solutions (, 0.11, and 0.24) and pure were investigated by Raman spectroscopy. Coupled and decoupled vibrational modes were identified at room temperature as a function of composition. Tetrahedral tilting librational modes involved in the displacive -quartz phase transition are decoupled. The wave number of the coupled mode located at for pure -quartz was found to vary quite linearly with germanium content. Raman spectra were recorded up to 1473 K. Substitution of germanium in the quartz lattice clearly improves the thermal stability of the phase. The -quartz phase transition temperature increases from for to about for . At the same time, the dynamic disorder observed in quartz well below the transition is reduced in the solid solutions.
Single crystals of α-quartz type Si1−xGexO2 with x < 0.2 were grown in 0.05 M NaOH solution. Infrared measurements confirmed that crystals grown at high pressure and high temperature have a low –OH group defect content. After a few millimeters of crystal growth under these conditions, α3500 reaches 0.1 cm−1 and no free –OH are present. The d11 value measured on an X-cut from the crystal with x = 0.0375 is 3.08 pC N−1 (±0.15), in good agreement with the value of 2.97 pC N−1 obtained using density functional theory based calculations. Piezoelectric measurements were performed on the Si1−xGexO2 crystal with x = 0.0375, both at room temperature and after annealing at various temperatures. The piezoelectric signal of the crystal with x = 0.0375 and pure SiO2 disappears after annealing at 635 °C and 545 °C, respectively. Nonlinear optical (NLO) properties of Si1−xGexO2 crystals were measured by Maker's fringe technique on Z-cut χ11(2) and their corresponding values for x = 0.023 and 0.028 are 1.3(2) pm V−1 and 1.6(2) pm V−1, respectively. These values are in good agreement with density functional theory based calculations. The light induced damage threshold values measured on Si1−xGexO2 crystals with x = 0.023 and 0.028 are very similar to that of α-quartz.