The effect of Cu addition and the intercritical annealing (IA) temperature on the microstructural evolution and mechanical properties of Fe-0.4C-7Mn-4Al (wt%) was investigated via scanning electron microscopy (SEM), electron backscatter diffraction (EBSD), X-ray diffraction (XRD) and nanoindentation tests. The results showed that the volume fraction and the average grain size of austenite, and the fraction of high angle grain boundaries, increased with IA temperature increase in the range of 650 °C to 710 °C. The addition of Cu facilitates the formation of Cu-rich nanoparticles, raises the volume fraction of austenite, and delays the recrystallization of austenite. As IA temperature increased, the yield strength (YS), ultimate tensile strength (UTS), and Lüders bands strain (LBS) decreased in both experimental steels. The Cu addition not only increases the YS of medium Mn steel but also benefits the decrease of LBS. The best comprehensive mechanical properties were obtained at the IA temperature of 690 °C in the studied steel, with Cu addition. According to nanoindentation experiments, the Cu addition raises the hardness of ferrite and austenite from 4.7 GPa to 6.3 GPa and 7.4 GPa to 8.5 GPa, respectively, contributing to the increase of YS of medium-Mn steel.
19 February 2026 in Materials Science and Engineering: A
Mircowave absorption materials can solve the problem of electromagnetic pollution, but corrosion in harsh environments will lead to a decrease in its absorption performance, so it is important to study materials that are both mircowave absorption and corrosion-resistant. In this experiment, FeSiAl alloy was coated Al2O3 (noted as FeSiAl@ Al2O3 coating) with aluminum chloride hexahydrate as aluminum source, and its mircowave absorption and corrosion resistance properties were studied. The results show that the mircowave absorption and corrosion resistance performance of FeSiAl@ Al2O3 coating both are obviously improved. The minimum reflection loss of FeSiAl@Al2O3 is -43.4 dB, the matching thickness is 2.3 mm, and the effective bandwidth is 2.97 GHz. For the coated alloy, the corrosion current decreases from 3.538*10-4 A/cm2 to 3.499*10-4 A/cm2, and the corrosion resistance increases from 96.1 ohm to 225.1 ohm. This provides an effective way to develop iron aluminum silicon materials that combine microwave absorption and corrosion resistance.
Hot compression experiments were performed to characterize the high-temperature deformation behavior of CoNiV medium-entropy alloy (MEA). Hot compression tests were carried out using a Gleeble-3500 thermomechanical simulator over strain rates of 0.001 s−1 to 1 s−1 and temperatures ranging between 950 °C and 1100 °C. Based on the experimentally determined hot compression data, three models for predicting the flow stress of CoNiV MEA were established: the Zerilli-Armstrong (Z-A) constitutive model, an artificial neural network (ANN) model, and a gated recurrent unit (GRU) model. This study comprehensively evaluated the prediction accuracy of each model using the coefficient of determination (R2), mean absolute error (MAE), and root mean square error (RMSE). The results show that, compared with the other two models, the Z-A model cannot accurately predict the flow behavior of CoNiV MEA in the studied hot-working regime. The R2 value of the ANN model is 0.98974, while the GRU model exhibits the highest predictive capability, with an R2 value of 0.98981, an MAE of 6.29621, and an RMSE of 13.10832. The proposed model demonstrates superior prediction accuracy compared with other models, enabling high-precision characterization of the high-temperature evolution of the flow stress in the CoNiV MEA. This study provides a theoretical foundation for the design and optimization of hot working parameters for the CoNiV MEA.
In this study, a multi-gradient microstructure was introduced into medium-Mn steel through torsion following heat treatment at different annealing temperatures, and through investigations on the mechanical properties under two annealing temperatures, it has also been revealed that different annealing temperatures before torsion affect the stability of austenite after torsion, thereby leading to distinct variations in mechanical performance. The yield strengths of the studied steel after annealing at 600 °C and 620 °C were 762 MPa and 673 MPa, with total elongation of 47.4% and 44.1%, respectively. After 90° torsion, the yield strength of experimental steels increased to 834 MPa and 808 MPa, while the elongation decreased to 21.6% and 29.5%, respectively. The gradient distributions from the center to the edge were observed for the austenite volume fraction, average grain size, martensite volume fraction, GND density, and hardness. The comparative analysis of the two annealing temperatures indicates that the larger grain size in the 620—annealed sample leads to its lower yield strength, while its higher austenite volume fraction and moderate stability promote a more sustained TRIP effect during deformation, contributing to its enhanced elongation. This multi-gradient microstructure is responsible for the yield strength improvements of 72 MPa and 135 MPa in the torsioned samples annealed at 600 °C and 620 °C, respectively.